The technology of salt carving and tail salt is applied in the field of preparation of salt carving handicrafts, which can solve the problems of long storage time of salt carving works, reduced product scrap rate and high ornamental value, and achieves good industrial application prospects, long ornamental life and engraving. Good results
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] Step 1, in a dust-free workshop, take commercially available sea salt and add deionized water to dissolve to obtain a saturated solution, filter to remove insoluble matter such as sediment; step 2, add citric acid with a purity of 95% or more to the saturated solution in step 2, and stir until Precipitation appears, filter, and take the clear liquid; step 3, use steam to heat and concentrate the solution obtained in step 3 at 60-70°C to a paste state, the water content is less than 8%, fully stir with epoxy resin and curing agent M50, and then inject In the mold, vacuumize, pressurize, solidify and shape; step 5, demoulding, drying, grinding, modifying corners, polishing, until the product is smooth, and the finished product is obtained.
Embodiment 2
[0019] Step 1: Take the industrial tailing salt from a potash fertilizer plant and calcinate it in a tunnel kiln at 500-550° C. for 20-30 minutes in a corundum container. Cool, add deionized water to dissolve and heat to 70-80°C, stir, filter while it is hot, concentrate by vacuum distillation, cool down, and crystallize to obtain crystals; step 2, in a dust-free workshop, dissolve the crystals obtained in step 1 in deionized In water, obtain a saturated saline solution, filter to remove insoluble impurities; step 3, add citric acid with a purity of 95% or more to the saturated solution in step 2, stir until precipitation occurs, filter, and take the clear liquid; step 4, use the solution obtained in step 3 The steam is heated and concentrated at 60-70°C until it becomes a paste, and the water content is less than 10%. After fully stirring with epoxy resin and curing agent M50, it is injected into the mold, vacuumed, pressurized and solidified; step 5, demoulding, Drying, grin...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com