Embodiment 1
[0042] The wheat seed coating agent is made of the following raw materials: 32 parts of fludioxonil (10%), 32 parts of metalaxyl powder (35%), 5 parts of boric acid, 5 parts of borax, 10 parts of magnesium sulfate, and 1.8 parts of paclobutrazol , 0.2 parts of algin oligosaccharide, 4 parts of polyvinyl alcohol, 5 parts of sodium carboxymethylcellulose (CMC), 4 parts of rhodamine, compound type of styrene-based phenol polyoxyethylene ether and calcium dodecylbenzenesulfonate 1 part emulsifier.
[0043] The method for preparing wheat seed coating agent, comprises the steps:
[0044] 1) Mix fludioxonil and metalaxyl powder, and ball mill to obtain component A;
[0045] 2) Mix other raw materials, add them to the ball mill of component A, and continue ball milling to obtain mixed raw materials with a fineness of 400-500 mesh, which is component B;
[0046] 3) Put component B into a jet mill for ultrafine pulverization for 15-30 minutes until it reaches 1000 mesh.
[0047] In s...
Embodiment 2
[0052] The wheat seed coating agent is made of the following raw materials: 30 parts of fludioxonil (10%), 34 parts of metalaxyl powder (35%), 5 parts of boric acid, 5 parts of borax, 10 parts of magnesium sulfate, and 1.8 parts of paclobutrazol , 0.2 parts of algin oligosaccharide, 4 parts of polyvinyl alcohol, 5 parts of sodium carboxymethyl cellulose (CMC), 4 parts of rhodamine, compound type of styrylphenol polyoxyethylene ether and calcium dodecylbenzenesulfonate 1 part emulsifier.
[0053] The preparation method is the same as in Example 1.
[0054] Mix well with wheat seeds at a ratio of 1:800.
[0055] The test showed that: compared with the control without seed dressing, the germination rate of wheat increased by 18.33%, and compared with the control of domestic and imported seed coating agents, the germination rate increased by 7.82% and 2.63% respectively; The number and 1,000-grain weight were also higher than those of the non-dressing control, domestic and impor...
Embodiment 3
[0057] Wheat seed coating agent, made from the following raw materials: 28 parts of fludioxonil (10%), 36 parts of metalaxyl powder (35%), 5 parts of boric acid, 5 parts of borax, 10 parts of magnesium sulfate, 1.8 parts of paclobutrazol , 0.2 parts of algin oligosaccharide, 4 parts of polyvinyl alcohol, 5 parts of sodium carboxymethyl cellulose (CMC), 4 parts of rhodamine, compound type of styrylphenol polyoxyethylene ether and calcium dodecylbenzenesulfonate 1 part emulsifier.
[0058] Preparation method is with embodiment 1.
[0059] Mix well with wheat seeds at a ratio of 1:800.
[0060] Under the application condition of this kind of coating agent, compared with the control without seed dressing, the germination rate of wheat increased by 16.37%, the ear grain weight increased by 16.9%, the disease index of take-all disease decreased by 27.75%, and the disease control effect reached 64.34%. Under the test of this seed coating agent, the average yield of wheat per mu was...