Embodiment 1
[0036] The polyacrylonitrile spinning stock solution using NaSCN aqueous solution as solvent was prepared by the usual method. The composition of polyacrylonitrile is: 91.5% of acrylonitrile, 7.0% of methyl acrylate, and 1.5% of sodium methacrylate. The concentration of polyacrylonitrile in the spinning dope is 13%, and the concentration of NaSCN is 45%. APP (polymerization degree 200, Jiangsu Zhenjiang Xingxing Flame Retardant Factory) with 15% polyacrylonitrile content was mixed with the above-mentioned NaSCN aqueous solution to obtain APP slurry. Stir and mix the obtained slurry with the spinning dope, first stir at room temperature for 10 minutes, then raise the temperature to 45°C at a heating rate of 2.5°C / min under stirring, and then raise the temperature to 65°C at a heating rate of 1.5°C / min, And continue to stir at this temperature for 15 minutes, and obtain the blended spinning stock solution through defoaming. Using a spinneret with a spinneret diameter of Φ0.06m...
Embodiment 2
[0040] Others are the same as in Example 1, except that APP has been surface-treated with KH550 in advance. The blended spinning dope has good spinnability, the obtained fiber has a fineness of 2.2dtex, a breaking strength of 2.5cN / dtex, a breaking elongation of 29%, and an LOI of 26.4.
Embodiment 3
[0042] Others are the same as in Example 2, except that PER is added in the blended spinning stock solution. The amount of PER is 40% of APP. The blended spinning dope has good spinnability, the resulting fiber has a fineness of 2.3dtex, a breaking strength of 2.4cN / dtex, a breaking elongation of 29%, and an LOI of 27.5.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
degree of polymerization | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com