Surface treatment solution for manufacturing solid electrolytic capacitor

A solid electrolysis and surface treatment technology, applied in the direction of solid electrolytic capacitors, etc., can solve the problems of unfavorable large-scale industrial production, failure to meet high performance requirements, and low capacity pass rate, etc., and achieve significant economic and social benefits and protection effects Excellent, high leakage pass rate effect

Inactive Publication Date: 2010-09-01
FUJIAN GUOGUANG ELECTRONICS SCI & TECHCO
View PDF3 Cites 15 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0004] When producing solid electrolytic capacitors in the prior art, chemical polymerization or chemical polymerization and electrochemical polymerization are directly used to prepare the conductive layer on the oxide film medium, so that the capacity of the capacitor produced in this way is often small, and the ESR is large, which cannot Meet high performance requirements
[0005] The Chinese invention application No. CN1832073 published on 2006.09.13 discloses a technical solution for manufacturing solid electrolytic capacitors by using coupling agent treatment. The capacity has been significantly improved, but the extraction rate is still not too high, and the capacity pass rate It is not very high in actual production, which is very unfavorable for large-scale industrial production

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0017] Taking a solid aluminum electrolytic capacitor as an example, an oxide film dielectric aluminum oxide is formed on the surface of the aluminum core of the anode body, the surface of the aluminum oxide is impregnated with a surface treatment solution to form a treatment layer, and then a solid electrolyte layer is formed on the surface of the treatment layer. A first cathode layer is formed on the outer surface of the first cathode layer; a second cathode layer is formed on the outer surface of the first cathode layer to obtain a monolithic capacitor element, and then the capacitor element is assembled and packaged to obtain a solid aluminum electrolytic capacitor.

[0018] The surface treatment solution consists of silane coupling agent, methanol organic solvent, deionized water and fluorine-containing nonionic surfactant. Wherein the mass concentration of silane coupling agent is 0.001%, the mass concentration of fluorine-containing nonionic surfactant is 0.001%, the ma...

Embodiment 2

[0023] The oxide film medium aluminum oxide is formed on the surface of the aluminum core of the anode body of the solid aluminum electrolytic capacitor, and the surface treatment solution is sprayed on the surface of the aluminum core to form a treatment layer, and then a solid electrolyte layer is formed on the surface of the treatment layer. In the solid electrolyte A first cathode layer is formed on the outer surface of the first cathode layer; a second cathode layer is formed on the outer surface of the first cathode layer to obtain a monolithic capacitor element, and then the capacitor element is assembled and packaged to obtain a solid aluminum electrolytic capacitor.

[0024] The surface treatment solution consists of silane coupling agent, acetone organic solvent, deionized water and NP-10 surfactant. Wherein the mass concentration of silane coupling agent is 50%, the mass concentration of NP-10 surfactant is 0.5%, the mass concentration of deionized water is 10.0%, an...

Embodiment 3

[0028] Take solid tantalum capacitors as an example. Sinter the tantalum powder compact to obtain the anode body tantalum block, form an oxide film medium tantalum pentoxide on the surface of the tantalum block, then brush the surface treatment solution on the surface of the tantalum pentoxide to form a treatment layer, and form a solid electrolyte on the surface of the treatment layer. A first cathode layer is formed on the outer surface of the solid electrolyte layer; a second cathode layer is formed on the outer surface of the first cathode layer to obtain a capacitor element, and then the capacitor element is assembled and packaged to obtain a solid tantalum capacitor.

[0029] The surface treatment solution is composed of aluminate coupling agent, ether organic solvent, deionized water and phosphate ester salt type surfactant. Wherein the mass concentration of aluminate coupling agent is 20%, the mass concentration of phosphate ester salt type surfactant is 1%, the mass c...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention provides surface treatment solution for manufacturing a solid electrolytic capacitor, which at least comprises a coupling agent for connecting an anode body surface oxide film medium with a solid electrolyte in the solid electrolytic capacitor, wherein the surface treatment solution also comprises a surfactant for reducing the surface tension of solution of the coupling agent, and improving the effect of the solution of the coupling agent for wetting the anode body surface oxide film medium to ensure that the coupling agent is more uniformly covered on the surface of the anode body surface oxide film medium, so the bonding between the anode body surface oxide film medium and the solid electrolyte is more uniform, and the bonding area and the bonding strength are improved.

Description

【Technical field】 [0001] The invention relates to a solid electrolytic capacitor, in particular to a surface treatment solution for making a solid electrolytic capacitor. 【Background technique】 [0002] With the continuous development of science and technology, the market increasingly needs capacitors with small size, large capacity, low loss, low ESR, and high reliability. One of the ways to improve the performance of capacitors is to improve the conductivity, regularity, and stability of solid electrolytes. sex, flatness. In the production process, chemical oxidation or electrolytic oxidation polymerization is generally used to polymerize pyrrole, aniline, thiophene or its derivative monomers to form a solid electrolyte for electrolytic capacitors. Since the oxide film medium on the surface of the anode body and the solid electrolyte are two materials with different properties, it is difficult for the monomer of the solid electrolyte to attach to the surface of the oxide ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): H01G9/15
Inventor 张易宁何腾云
Owner FUJIAN GUOGUANG ELECTRONICS SCI & TECHCO
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products