Environment-friendly dendritic polyether dirt dispersion agent and preparation method thereof
The technology of scale inhibitor and dispersant and dendritic polyether is applied in the field of high calcium cooling water quality, which can solve the problems of secondary pollution and increase the cost of industrial application, and achieve low production cost, good biodegradation performance, and a green environment for the preparation process. friendly effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
example 1
[0018] Example 1: in N 2 Add 120g of allyl polyethylene glycol monoether to the protected reactor, add 10g of NaOH to alkalinize at 65°C for 3h, add 60g of glycidyl alcohol at 80°C for 6h; adjust the temperature to 75°C, add 100g of acrylic acid, 100g of water, mix well, add potassium persulfate (15g) (dissolved in 100g of water) dropwise, after 3 hours of dropwise addition, raise the temperature to 80°C and continue the reaction for 5 hours, after cooling down to room temperature, an environmentally friendly dendrimer Ether antiscalant dispersant (APELL).
[0019] When the obtained APELL dosage is 6mg / L, the Ca 3 (PO 4 ) 2 Scale inhibition rate up to 99.9%, for CaCO 3 Scale inhibition rate is 92.1%, for CaSO 4 The scale inhibition rate is 96.8%, and the light transmittance of the solution containing Fe(III), which characterizes the performance of dispersing iron, is 15.2%.
example 2
[0020] Example 2: in N 2 Add 100g of allyl polyethylene glycol monoether to the protected reactor, add 20g of KOH to alkalinize at 55°C for 3h, add 50g of glycidyl alcohol and react at 80°C for 6h; after adjusting the temperature to 75°C, add 100g maleic anhydride, 220g water, mix well, add potassium persulfate (10g) (dissolved in 180g water) dropwise, after 2h dropwise addition, raise the temperature to 90°C and continue the reaction for 4h, after cooling down to room temperature, the environmentally friendly branch Polyether antiscalant dispersant (APELL).
[0021] When the obtained APELL antiscalant was added at 8mg / L, the effect on Ca 3 (PO 4 ) 2 Scale inhibition rate up to 99.6%, for CaCO 3 Scale inhibition rate is 90.5%, for CaSO 4 The scale inhibition rate is 95.3%. , the light transmittance of the Fe(III)-containing solution, which characterizes the performance of dispersing iron, is 17.1%.
example 3
[0022] Example 3: in N 2 Add 180g allyl polyethylene glycol monoether in the reactor of protection, add 25gCH 3 CH 2 After basifying ONa at 55°C for 3 hours, add 180g glycidol and react at 80°C for 8h; after adjusting the temperature to 75°C, add 80g acrylic acid, 80g maleic anhydride, 200g water, mix well and add persulfuric acid dropwise Potassium (5g), sodium persulfate (10g) mixture (dissolved in 240g water), after 3 hours of dropwise addition, the temperature was raised to 80°C to continue the reaction for 6 hours, and after cooling down to room temperature, an environmentally friendly dendritic polyether scale inhibitor dispersant was prepared (APELL).
[0023]When the obtained APELL scale inhibitor is added at 6mg / L, the effect on Ca 3 (PO 4 ) 2 Scale inhibition rate can reach 97.4%, for CaCO 3 Scale inhibition rate is 90.3%, for CaSO 4 The scale inhibition rate is 95.8%, and the light transmittance of the solution containing Fe(III), which characterizes the p...
PUM
Property | Measurement | Unit |
---|---|---|
degree of polymerization | aaaaa | aaaaa |
degree of polymerization | aaaaa | aaaaa |
transmittivity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com