Sewage treatment agent
A wastewater treatment agent, volcanic stone technology, applied in biological water/sewage treatment, water/sludge/sewage treatment, water pollutants, etc. Achieve the effect of stable chemical properties, low processing cost and good adsorption capacity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] A waste water treatment agent, in parts by weight, mainly made of the following raw materials: 20 parts of aluminum sulfate, 23 parts of iron sulfate, 3 parts of polyacrylamide, 4 parts of microorganisms, 22 parts of potato starch, 8 parts of sodium polyacrylate, 11 parts of bentonite, 7 parts of tannin, 8 parts of potassium permanganate and 30 parts of modified volcanic stone.
[0020] The preparation method of described modified volcanic stone is as follows:
[0021] (1) pretreatment of the volcanic stone, drying the volcanic stone at a temperature of 90-100°C for 15 hours; then calcining the volcanic stone at a temperature of 550-600°C for 2.5 hours;
[0022] (2) Modification of volcanic stone: after the volcanic stone after step (1) is calcined is cooled, add volcanic stone to 35% hydrochloric acid solution and 20% dopamine hydrochloride mixed solution and carry out soaking reaction 3-5h, 35% The volume ratio of hydrochloric acid solution and 20% dopamine hydrochlo...
Embodiment 2
[0029] A wastewater treatment agent, in parts by weight, mainly made of the following raw materials: 15 parts of aluminum sulfate, 30 parts of iron sulfate, 1 part of polyacrylamide, 5 parts of microorganisms, 15 parts of potato starch, 3 parts of sodium polyacrylate, 7 parts of bentonite, 10 parts of tannin, 4 parts of potassium permanganate and 40 parts of modified volcanic stone.
[0030] The preparation method of described modified volcanic stone is as follows:
[0031] (1) pretreatment of the volcanic stone, drying the volcanic stone at a temperature of 90-100°C for 20 hours; then calcining the volcanic stone at a temperature of 550-600°C for 2 hours;
[0032] (2) Modification of volcanic rock: after the volcanic rock after the calcining in step (1) is cooled, add volcanic rock to 35% hydrochloric acid solution and 20% dopamine hydrochloride mixed solution to carry out soaking reaction for 3h, 35% hydrochloric acid solution The volume ratio of mixing with 20% dopamine hy...
Embodiment 3
[0039] A waste water treatment agent, in parts by weight, mainly made of the following raw materials: 30 parts of aluminum sulfate, 15 parts of iron sulfate, 5 parts of polyacrylamide, 1 part of microorganisms, 30 parts of potato starch, 13 parts of sodium polyacrylate, 17 parts of bentonite, 5 parts of tannin, 11 parts of potassium permanganate and 20 parts of modified volcanic stone.
[0040] The preparation method of described modified volcanic stone is as follows:
[0041](1) pretreatment of the volcanic stone, drying the volcanic stone at a temperature of 90-100°C for 10 hours; then calcining the volcanic stone at a temperature of 550-600°C for 3 hours;
[0042] (2) Modification of volcanic stone: after the volcanic stone after step (1) is calcined is cooled, add volcanic stone to 35% hydrochloric acid solution and 20% dopamine hydrochloride mixed solution and carry out soaking reaction 5h, 35% hydrochloric acid solution The volume ratio of mixing with 20% dopamine hydro...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com