An analgesic cold compress and its preparation process
A preparation process and technology of sodium polyacrylate, applied in the field of medical devices, can solve the problems of inability to exert analgesic effect, unsatisfactory analgesic effect, waste of drugs and the like
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0036] A preparation process of analgesic cold compress, the specific method is: firstly add the first part of sodium polyacrylate, glycerol, crospovidone, polymethacrylic acid and iron oxide black into glycerin to make an oil phase; Then tartaric acid, preservatives, the second part of sodium polyacrylate, traditional Chinese medicine extract, honey and water are mixed, supplemented with penetration enhancer, stabilizer, wintergreen oil, menthol and thermal agent to make the water phase; finally The oil phase and the water phase are vacuum mixed to obtain a hydrogel matrix, coated, cut, packaged, and solidified in a bag; wherein, the mass ratio of the first part of sodium polyacrylate to the second part of sodium polyacrylate is 5:3.
[0037] Specific steps are as follows:
[0038] (1) Add the first part of sodium polyacrylate, glycerol, crospovidone, polymethacrylic acid and iron oxide black into glycerin, and mix well to obtain an oil phase;
[0039] (2) After mixing the p...
Embodiment 2
[0054] A preparation process of analgesic cold compress, the specific method is: firstly add the first part of sodium polyacrylate, glycerol, crospovidone, polymethacrylic acid and iron oxide black into glycerin to make an oil phase; Then tartaric acid, preservatives, the second part of sodium polyacrylate, traditional Chinese medicine extract, honey and water are mixed, supplemented with penetration enhancer, stabilizer, wintergreen oil, menthol and thermal agent to make the water phase; finally The oil phase and the water phase are vacuum mixed to obtain a hydrogel matrix, coated, cut, packaged, and solidified in a bag; the mass ratio of the first part of sodium polyacrylate to the second part of sodium polyacrylate is 7:6.
[0055] Specific steps are as follows:
[0056] (1) Add the first part of sodium polyacrylate, glycerol, crospovidone, polymethacrylic acid and iron oxide black into glycerin, and mix well to obtain an oil phase;
[0057] (2) After mixing the penetratio...
Embodiment 3
[0072] A preparation process of analgesic cold compress, the specific method is: firstly add the first part of sodium polyacrylate, glycerol, crospovidone, polymethacrylic acid and iron oxide black into glycerin to make an oil phase; Then tartaric acid, preservatives, the second part of sodium polyacrylate, traditional Chinese medicine extract, honey and water are mixed, supplemented with penetration enhancer, stabilizer, wintergreen oil, menthol and thermal agent to make the water phase; finally The oil phase and the water phase are vacuum mixed to obtain a hydrogel matrix, coated, cut, packaged, and solidified in a bag; the mass ratio of the first part of sodium polyacrylate to the second part of sodium polyacrylate is 6:5.
[0073] Specific steps are as follows:
[0074] (1) Add the first part of sodium polyacrylate, glycerol, crospovidone, polymethacrylic acid and iron oxide black into glycerin, and mix well to obtain an oil phase;
[0075] (2) After mixing the penetratio...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com