Alcohol fuel additive and preparation method thereof
An additive and fuel technology, applied in the direction of fuel additives, fuel, petroleum industry, etc., can solve the problems of alcohol fuels not burning normally, poisoning and solubilization of three-way catalysts, and failing to be well solved, etc., and achieve excellent free radicals. and desulfurization performance, low working noise, stable working effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0047] Alcohol fuel additive, consisting of the following raw materials in parts by weight: 18 parts of fusel oil, 8 parts of trinitrophenol, 5 parts of potassium permanganate, 6 parts of dimethyl ether, 3 parts of methylamine, castor oil polyoxygen 3 parts of vinyl ether, 4 parts of 2,6-di-tert-butyl-p-cresol, 4 parts of tartaric acid.
[0048] The preparation method of above-mentioned alcohol fuel additive, comprises the steps:
[0049] (1) Weigh the fusel oil and the anti-oxidation and anti-adhesive agent according to the parts by weight, stir evenly, the temperature during the stirring process is 45°C, and the stirring time is 20min, to obtain the mixed solution A;
[0050] (2) Add a stabilizer to the mixed solution A obtained in step (1), stir evenly, the temperature during the stirring process is 50° C., and the stirring time is 10 minutes to obtain a mixed solution B;
[0051] (3) Add an anti-swelling agent and a neutralizing agent to the mixed solution B obtained in s...
Embodiment 2
[0061] Alcohol fuel additive, made up of the following raw materials in parts by weight: 15 parts of fusel oil, 11 parts of trinitrophenol, 8 parts of isopropanol, 3 parts of triphenylamine, 4 parts of lecithin, 3 parts of tartaric acid; 2,6 - 5 parts of di-tert-butyl-p-cresol.
[0062] The preparation method of above-mentioned alcohol fuel additive, comprises the steps:
[0063] (1) Weigh the fusel oil and the anti-oxidation and anti-adhesive agent according to the parts by weight, stir evenly, the temperature during the stirring process is 40°C, and the stirring time is 20min, to obtain the mixed solution A;
[0064] (2) Add a stabilizer to the mixed solution A obtained in step (1), stir evenly, the temperature during the stirring process is 45° C., and the stirring time is 10 minutes to obtain the mixed solution B;
[0065] (3) Add an anti-swelling agent and a neutralizing agent to the mixed solution B obtained in step (2), stir evenly, the temperature during the stirring ...
Embodiment 3
[0074] The alcohol fuel additive is composed of the following raw materials in parts by weight: 20 parts of fusel oil, 10 parts of potassium permanganate, 9 parts of dimethyl ether, 3-6 parts of methylamine, 2-5 parts of triethanolamine oleate, 3-5 parts of lactic acid; 2-6 parts of 2,6-di-tert-butyl-p-cresol.
[0075] The preparation method of above-mentioned alcohol fuel additive, comprises the steps:
[0076] (1) Weigh the fusel oil and the anti-oxidation and anti-adhesive agent according to the parts by weight, stir evenly, the temperature during the stirring process is 50°C, and the stirring time is 15min, to obtain the mixed solution A;
[0077] (2) Add a stabilizer to the mixed solution A obtained in step (1), stir evenly, the temperature during the stirring process is 40° C., and the stirring time is 12 minutes to obtain the mixed solution B;
[0078] (3) Add an anti-swelling agent and a neutralizing agent to the mixed solution B obtained in step (2), stir evenly, the...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com