Mesoporous silicon drug loading system, preparation method and mesoporous silicon loaded drug
A technology of mesoporous silicon and mesoporous silica, which is applied in the fields of pharmaceutical formulations, radioactive carriers, antineoplastic drugs, etc., can solve the problems of short loading time and difficulty in triggering the release of carriers, and achieves small drug impact, rapid assembly, Biocompatibility Biodegradable Effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0043] The mesoporous silicon drug loading system uses mesoporous silica as the carrier, the surface of the mesoporous silica is connected to cinnamaldehyde after surface amination treatment, and the gold nanoparticles coated with β-cyclodextrin are used as the mesoporous Silica pore blocking agent.
[0044] The mesoporous silicon drug-loading system described in this embodiment can be used to load drugs, including antitumor drugs (such as doxorubicin, pirarubicin hydrochloride, etc.), PET contrast agents (such as deoxyglucose-based contrast agents) 18 F-FDG, nitroimidazole hypoxic contrast agents 18 F-FMISO, etc.) and β-lactoglobulin, which can be used for multimodal imaging and targeted therapy of tumors, etc.
Embodiment 2
[0046] This embodiment is described with the loaded drug as doxorubicin (so the drug in this example is limited to doxorubicin):
[0047] A mesoporous silicon drug-carrying system comprises the mesoporous silicon drug-carrying system as described in Embodiment 1, wherein the mesoporous silicon drug-carrying system is loaded with a drug, and the drug comprises doxorubicin.
[0048] like figure 1 , figure 2 As shown, the specific preparation process of the mesoporous silicon drug loading described in this embodiment is as follows:
[0049] (1) Synthesis of Mesoporous Silicon Nanospheres (MSNS)
[0050] Take 32ml of cetyltrimethylammonium chloride / water solution with a mass fraction of 25%, add 88ml of deionized water, and then add 1.44ml of triethanolamine / water solution with a mass fraction of 25%, heat in an oil bath at 60 °C, as water Mutually. 40 ml of a 20% volume fraction of tetraethyl silicate / cyclohexane solution was freshly prepared and added to the water phase to ...
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 