A surface sizing agent, high-efficiency technology, applied in the field of papermaking additives, can solve the problems of unsatisfactory sizing effect of surface sizing agent, easy hydrolysis of sizing agent in pulp, high cost of sewage treatment, etc., and achieve excellent sizing effect , Reduce the requirements of the slurry purification system, and the effect of less foaming
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] Example 1: first pour 45 parts of water (100 parts in total, each part is 100 g, the same below) into a reaction kettle and heat to 75 ° C, then melt 18 parts of solid alkyl ketene dimer at high temperature, Under the condition of continuous stirring, put it into the reaction kettle and fully mix it with water, then add 18 parts of starch and acrylamide graft copolymer, and continue stirring for 30 minutes to obtain an emulsion; then add 11 parts of polyamide amide resin to the emulsion, 8 parts of methacryloyloxyethyltrimethylammonium chloride, after stirring evenly, homogenize through a high-pressure homogenizer, and become a high-efficiency surface sizing agent product after cooling down.
Embodiment 2
[0018] Example 2: first pour 50 parts of water (100 parts in total, each part is 100 g, the same below) into the reaction kettle and heat to 75 ° C, then melt 16 parts of solid alkyl ketene dimer at high temperature, Under the condition of continuous stirring, put it into the reactor and mix it fully with water, then add 18 parts of starch and acrylamide graft copolymer, and stir for 30 minutes to obtain an emulsion; then add 10 parts of polyamide amide resin to the emulsion, 8 Dodecyltrimethylammonium chloride, after stirring evenly, homogenize through a high-pressure homogenizer, and become a high-efficiency surface sizing agent product after cooling down.
Embodiment 3
[0019] Example 3: first pour 55 parts of water (100 parts in total, each part is 100 g, the same below) into the reactor and heat to 75 ° C, then melt 14 parts of solid alkyl ketene dimer at high temperature, Under the condition of continuous stirring, put it into the reaction kettle and mix it fully with water, then add 15 parts of starch and acrylamide graft copolymer, and stir for 30 minutes to obtain an emulsion; then add 10 parts of polyethyleneimine resin to the emulsion, 6 parts of tetradecyltrimethylammonium chloride, after stirring evenly, homogenize through a high-pressure homogenizer, and become a high-efficiency surface sizing agent product after cooling down.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com