Texture coating and preparation method thereof
A textured coating and aggregate technology, applied in the field of coatings, can solve problems such as poor weather resistance, and achieve the effects of good wear resistance, good frost resistance and high strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0028] 3. The preparation process of acid hydrolyzed hydroxypropyl starch is as follows: in deionized water, add a swelling inhibitor relative to the starch mass ratio of 13%, add sodium hydroxide accounting for 1.0% of the starch mass, mix and stir until dissolved, and add the step (1) Adjust the prepared acid-thinned starch into 35% starch milk, stir and alkalinize for 40 minutes, heat up to 42°C, add propylene oxide accounting for 5% of the starch mass, etherify for 14 hours, add 10% hydrochloric acid to adjust the pH to 7.0, after centrifugal dehydration, drying and sieving, the acid hydrolyzed hydroxypropyl starch can be obtained;
[0029] 4. The preparation process of acid-thinned starch used in the preparation process of acid-thinned carboxymethyl starch and acid-thinned hydroxypropyl starch is as follows: add HCl solution with a mass percentage concentration of 0.6% to the starch, and prepare starch with a concentration of 38%. Milk, heated to 50°C, acidolysis for 2 ho...
Embodiment 1
[0035] Example 1. Aggregate (red) for texture paint preparation:
[0036] The amount of raw materials for the aggregate is as follows: 50 kg of cement, 10 kg of lime, 15 kg of gypsum, 10 kg of fine sand (100 mesh), 20 kg of biomass binder, 8 kg of red water-based color paste, and 8 kg of demineralized water.
[0037] Aggregate preparation method:
[0038] a) Mix the water-based color paste and the biomass binder uniformly in parts by mass to obtain a mixed solution, which is set aside;
[0039] b) Add cement, lime, gypsum and fine sand into the mixer in parts by mass, and stir the mixture evenly;
[0040] c) Add the mixture obtained in step b to the water-based color paste and binder mixture prepared in step a, and stir well; d) Granulate the substance obtained in step c with a rotary granulator to prepare a granule with a particle size of 2.5 mm. Granules, dried, sized and sieved to obtain aggregate.
Embodiment 2
[0041] Example 2. Preparation of aggregate (yellow) for textured paint
[0042] The amount of raw materials for aggregate is as follows: 50 kg of cement, 15 kg of lime, 10 kg of gypsum, 5 kg of fine sand (100 mesh), 20 kg of biomass binder, 5 kg of yellow water-based color paste, and 10 kg of demineralized water.
[0043] Aggregate preparation method:
[0044] a) Mix the water-based color paste and the biomass binder uniformly in parts by mass to obtain a mixed solution, which is set aside;
[0045] b) Add cement, lime, gypsum and fine sand into the mixer in parts by mass, and stir the mixture evenly;
[0046] c) Add the mixture obtained in step b to the water-based color paste and binder mixture prepared in step a, and stir well; d) Granulate the substance obtained in step c with a rotary granulator to prepare granules with a particle size of 0.2 mm. Granules, dried, sized and sieved to obtain aggregate.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com