Preparation method of silver product with colored surface
A technology of silver products and colors, applied in the direction of metal material coating process, etc., can solve the problems of yellowing and blackening of silver edges, loss of value, and failure of glaze to completely cover silver tires.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0024] The invention provides a kind of preparation method of the silver product with color on the surface, comprises the following steps:
[0025] The surface of the degreased silver product is reacted with a coloring agent to obtain a silver product with a colored surface.
[0026] The invention utilizes the active chemical properties of silver to reflect different coloring reagents on the surface of silver products, so that the silver on the surface of silver products reacts with the coloring reagents to obtain reaction products of different colors, so that the surface of silver products presents different colors . In the present invention, preferably, potassium sulfide and ammonium chloride are used as the coloring reagent, the coloring reagent is reacted with the surface of the silver product, and the reaction product silver sulfide of jazz silver is obtained on the surface of the silver product, and the silver sulfide will be complexed The reaction forms a complex, whic...
Embodiment 1
[0049] At 8°C, place the silver product to be treated in a degreasing solution, which includes 5g / L of sodium carbonate, 2g / L of sodium hydroxide and 15g / L of washing spirit, and repeatedly smear and wipe the metal with absorbent cotton Rinse the surface with water until the metal surface shows a continuous water film to complete the degreasing of silver products;
[0050] Dissolve 1g of potassium sulfide and 1g of ammonium chloride in 10mL of water to obtain a colored solution;
[0051] Immerse the degreased silver product in the coloring solution, react for 5 minutes, smear sodium bicarbonate on the obtained silver product, and wipe it to obtain the silver product of jazz silver;
[0052] After finishing the coloring of the silver product, the silver product on the surface of the jazz silver obtained is cleaned with clear water, and the cleaned silver product is dried with a hair dryer at a temperature of 50° C.;
[0053] Put the dried silver product on the rotary turntable...
Embodiment 2
[0057] At 5°C, place the silver product to be treated in a degreasing solution, which includes 2g / L sodium carbonate, 5g / L sodium hydroxide and 20g / L washing spirit, and repeatedly smear and wipe the metal with absorbent cotton Rinse the surface with water until the metal surface shows a continuous water film to complete the degreasing of silver products;
[0058] Dissolve 2g of potassium sulfide and 5g of ammonium chloride in 25mL of water to obtain a colored solution;
[0059] Immerse the degreased silver product in the coloring solution, react for 8 minutes, smear sodium bicarbonate on the surface of the obtained silver product, and wipe it to obtain the silver product of jazz silver; after finishing the coloring of the silver product, the obtained Clean the silver products on the surface of jazz silver with clean water, and dry the cleaned silver products with a hair dryer at a temperature of 40°C;
[0060] Put the dried silver product on the rotary turntable, and spray t...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com