Wear-resistant metal nickel ceramic coating layer for pot and manufacture method thereof
A wear-resistant metal and ceramic coating technology, used in coatings, metal-free paints, etc., can solve the problems of unfavorable energy-saving and green development, low toughness, and high cost, and can strengthen the interaction of atomic orbitals, improve adhesion, The effect of improving wear resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0012] The wear-resistant metal nickel ceramic coating for a pot is characterized in that it is made of the following raw materials in parts by weight: nano cerium dioxide 15, nickel powder 42, iron powder 14, boron oxide 18, antimony trioxide 14. PTFE wax powder 9, aluminum dihydrogen phosphate 10, hydrogenated silicone oil 8, steel fiber 6, pure benzene emulsion 15, kaolin 23, appropriate amount of water.
[0013] The preparation method comprises the following steps:
[0014] (1) Treat nano ceria at 620-740°C for 30-50 minutes at high temperature, quickly cool to room temperature with liquid nitrogen, add aluminum dihydrogen phosphate and ultrasonically shake for 20-40 minutes, add pure benzene emulsion and stir to mix, Stir for 5-8h, dry to constant weight;
[0015] (2) Add boron oxide into a ball mill, spray into mist hydrogenated silicone oil and mix well, add polytetrafluoroethylene wax powder, and perform ball milling, mixing, and dispersing at room temperature to obta...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com