Formaldehyde catching agent and preparation method thereof
A formaldehyde scavenger and raw material technology, applied in the field of air purification, can solve the problem of low formaldehyde absorption efficiency, and achieve the effects of good dispersibility, stable performance and simple preparation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] A formaldehyde trapping agent, its raw material components are composed of the following raw materials in parts by mass: 2 parts of sodium sulfite, 4 parts of hydrochloric acid, 20 parts of native starch slurry, 5 parts of sodium hydroxide, 3 parts of sodium sulfate, 2 parts of propylene oxide, 20 parts of nic acid, 3 parts of dicumyl hydroperoxide, 14 parts of deacetylated chitin, 4 parts of iron white powder, 10 parts of calcium carbonate powder, 4 parts of barium stearate, 14 parts of nitromethane, 11 parts of aniline, 9 parts of diatomite, 4 parts of alumina, 6 parts of diatomite composite catalyst, 10 parts of graphite powder, 8 parts of p-phenylenediamine, 4 parts of phenol, 20 parts of plant flower extract, 6 parts of ferric chloride and deionized 60 parts of water.
[0023] The preparation method of the above-mentioned formaldehyde scavenger comprises the following steps connected in sequence:
[0024] 1) Add sodium sulfite to 20wt% raw starch slurry and stir f...
Embodiment 2
[0029] A formaldehyde trapping agent, its raw material components are composed of the following raw materials in parts by mass: 6 parts of sodium sulfite, 8 parts of hydrochloric acid, 40 parts of native starch slurry, 10 parts of sodium hydroxide, 9 parts of sodium sulfate, 6 parts of propylene oxide, 25 parts of nic acid, 5 parts of dicumyl hydroperoxide, 17 parts of deacetylated chitin, 6 parts of iron white powder, 13 parts of calcium carbonate powder, 6 parts of barium stearate, 16 parts of nitromethane, 14 parts of aniline, 11 parts of diatomite, 6 parts of alumina, 8 parts of diatomite composite catalyst, 14 parts of graphite powder, 10 parts of p-phenylenediamine, 6 parts of phenol, 40 parts of plant flower extract, 8 parts of ferric chloride and deionized 100 parts of water.
[0030] The preparation method of the above-mentioned formaldehyde scavenger comprises the following steps connected in sequence:
[0031] 1) Add sodium sulfite to the 30wt% raw starch slurry an...
Embodiment 3
[0036] A formaldehyde scavenger, the raw material components are optimized in terms of parts by mass and consist of the following raw materials: 4 parts of sodium sulfite, 6 parts of hydrochloric acid, 30 parts of native starch slurry, 7 parts of sodium hydroxide, 6 parts of sodium sulfate, 4 parts of propylene oxide, 22 parts of tannic acid, 4 parts of dicumyl hydroperoxide, 15 parts of deacetylated chitin, 5 parts of iron white powder, 12 parts of calcium carbonate powder, 5 parts of barium stearate, 15 parts of nitromethane, 13 parts of aniline , 10 parts of diatomite, 5 parts of alumina, 7 parts of diatomite composite catalyst, 12 parts of graphite powder, 9 parts of p-phenylenediamine, 5 parts of phenol, 30 parts of plant flower extract, 7 parts of ferric chloride and 80 parts of ionized water.
[0037] The preparation method of the above-mentioned formaldehyde scavenger comprises the following steps connected in sequence:
[0038] 1) Add sodium sulfite to 20wt% raw star...
PUM
Login to View More Abstract
Description
Claims
Application Information