[0015] A kind of water-based composite paint for plastics, its raw material comprises 40 parts by weight of water-based chlorinated polyolefin resin, 20 parts of water-based acrylic resin, 30 parts of water-based polyurethane dispersion, 2 parts of silane coupling agent, 40 parts of nano-calcium carbonate, super 5 parts of fine talc powder, 20 parts of nano silicon dioxide, 5 parts of aluminum silicate, 6 parts of barium sulfate, 1 part of titanium dioxide, 4 parts of zinc phosphate, 1 part of adhesion promoter, 2.5 parts of dimethylethanolamine, leveling 1 part of antibacterial agent, 2 parts of antibacterial agent, 1 part of defoamer, 2 parts of antifungal agent, and 1 part of wetting agent.
Embodiment 2
[0017] A kind of water-based composite coating for plastics, its raw material comprises 20 parts by weight of water-based chlorinated polyolefin resin, 40 parts of water-based acrylic resin, 15 parts of water-based polyurethane dispersion, 5 parts of silane coupling agent, 20 parts of nano-calcium carbonate, super 10 parts of fine talc powder, 10 parts of nano silicon dioxide, 15 parts of aluminum silicate, 1 part of barium sulfate, 3 parts of titanium dioxide, 1 part of zinc phosphate, 4 parts of adhesion promoter, 0.5 parts of dimethylethanolamine, leveling 2 parts of antibacterial agent, 1 part of antibacterial agent, 2 parts of defoamer, 1 part of antifungal agent, and 2 parts of wetting agent.
Embodiment 3
[0019] A kind of water-based composite paint for plastics, its raw material comprises 30 parts by weight of water-based chlorinated polyolefin resin, 35 parts of water-based acrylic resin, 20 parts of water-based polyurethane dispersion, 4.5 parts of silane coupling agent, 30 parts of nano-calcium carbonate, super 8 parts of fine talc powder, 14 parts of nano silicon dioxide, 13 parts of aluminum silicate, 2 parts of barium sulfate, 2 parts of titanium dioxide, 2 parts of zinc phosphate, 2.6 parts of adhesion promoter, 2 parts of dimethylethanolamine, leveling 1.5 parts of antibacterial agent, 1.6 parts of antibacterial agent, 1.5 parts of defoamer, 1.5 parts of antifungal agent, and 1.8 parts of wetting agent.
[0020] The solid content of the water-based acrylic resin is 65%, and the particle diameter is 20-40nm.
[0021] The water-based polyurethane dispersion is prepared by the following process: mix isophorone diisocyanate, methylpropylene glycol, dimethylol propionic aci...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com