Novel environment-friendly building board
A technology for building panels and environmental protection, applied in the field of new environmentally friendly building panels, can solve the problems that building panels cannot meet performance requirements such as light weight, heat preservation, high strength, and environmental protection, and achieve good performance and low energy consumption.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0033] The preparation method of the novel environmentally friendly building board comprises the following steps:
[0034] S1: mix cement, hydrogen peroxide, glyoxal and water evenly at a rotating speed of 100-300r / min to prepare slurry;
[0035] S2: Combine shale ore, fly ash, tailings sand, bentonite, kaolin, paraffin, sulfomethyl phenolic resin, AR glass fiber, carboxymethyl cellulose, water reducing agent, foaming agent, foaming regulator , catalyst, cross-linking agent and foam stabilizer are stirred for 3-4 hours at a temperature of 200-300 ° C and a rotating speed of 60-100 r / min to obtain a foam liquid;
[0036] S3: adding the foam liquid prepared in step S2 to the slurry prepared in step S1, and stirring evenly at a rotational speed of 200-300 r / min to prepare a foaming material;
[0037] S4: pour the foamed material obtained in step S3 into a mold, vibrate and smooth it, and apply a pressure of 0.9-0.95MPa to the foamed material for molding for 12-15s, and demold to...
Embodiment 1
[0041] A new type of environmentally friendly building board, in parts by weight, comprising the following raw materials: 30 parts of cement, 5 parts of shale ore, 2.5 parts of fly ash, 1.6 parts of tailing sand, 1.5 parts of bentonite, 1.5 parts of kaolin, and 3 parts of paraffin parts, 4 parts of sulfomethyl phenolic resin, 2.5 parts of AR glass fiber, 2.5 parts of carboxymethyl cellulose, 0.9 part of water reducing agent, 0.5 part of foaming agent, 0.5 part of foaming regulator, 0.1 part of catalyst, cross-linking agent 0.5 part, 0.1 part of foam stabilizer, 20 parts of glyoxal, 15 parts of hydrogen peroxide, 230 parts of water;
[0042] The water reducing agent is a polycarboxylate water reducing agent;
[0043] The foaming agent is azodicarbonamide;
[0044] The foaming regulator is an acrylate foaming regulator;
[0045] The catalyst is stannous octoate;
[0046] The crosslinking agent is dicumyl peroxide;
[0047] The foam stabilizer is silicone amide;
[0048] The...
Embodiment 2
[0055] A new type of environmentally friendly building board, in parts by weight, comprising the following raw materials: 22 parts of cement, 4 parts of shale ore, 2 parts of fly ash, 1 part of tailings sand, 1 part of bentonite, 1 part of kaolin, and 2 parts of paraffin parts, 3 parts of sulfomethyl phenolic resin, 2 parts of AR glass fiber, 2 parts of carboxymethyl cellulose, 0.6 part of water reducing agent, 0.4 part of foaming agent, 0.4 part of foaming regulator, 0.1 part of catalyst, cross-linking agent 0.3 part, 0.1 part of foam stabilizer, 15 parts of glyoxal, 10 parts of hydrogen peroxide, 200 parts of water;
[0056] The water reducing agent is a polycarboxylate water reducing agent;
[0057] The foaming agent is azodicarbonamide;
[0058] The foaming regulator is an acrylate foaming regulator;
[0059] The catalyst is triethylenediamine hexahydrate;
[0060] The crosslinking agent is dicumyl peroxide;
[0061] The foam stabilizer is silicone amide;
[0062] The...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com