Embodiment 1
[0014] A hydrophobic soft tissue paper, comprising the following raw materials in parts by weight: 60 parts of coniferous wood, 40 parts of waste paper pulp, 20 parts of animal wax, 3 parts of dehydroabietic acid, 3 parts of dihydroabietic acid, tetrahydroabietic acid 3 parts of acid, 10 parts of esterified rosin, 15 parts of modified fuma rosin, 15 parts of maleic acid resin, 5 parts of acetic acid, 5 parts of polyoxyethylene sorbitan tristearate, 1-mercaptododecane 3 parts, 10 parts of dimethylaminoethyl methacrylate, 12 parts of potassium persulfate, 10 parts of cetyltrimethylammonium halide, 10 parts of acrylamide, 15 parts of stearic acid, 10 parts of edible alkali, borax 5 parts, 80 parts of deionized water.
[0015] Its preparation method includes the preparation of slurry and the application process of hydrophobic mixture. The raw material components of the slurry are coniferous wood will and waste paper pulp, and other substances are all hydrophobic mixtures. The appl...
Embodiment 2
[0017] A kind of hydrophobic soft tissue paper, comprising the following raw materials in parts by weight: 65 parts of coniferous wood, 45 parts of waste paper pulp, 25 parts of vegetable wax, 3 parts of dehydroabietic acid, dihydroabietic acid 3 parts of abietic acid, 3 parts of tetrahydroabietic acid, 15 parts of esterified rosin, 20 parts of modified fuma rosin, 17 parts of maleic acid resin, 8 parts of acetic acid, 10 parts of polyoxyethylene sorbitan tristearate , 3 parts of 1-mercaptododecane, 15 parts of dimethylaminoethyl methacrylate, 13 parts of potassium persulfate, 17 parts of cetyltrimethylammonium halide, 12 parts of acrylamide, 17 parts of stearic acid parts, 13 parts of edible alkali, 7 parts of borax, and 100 parts of deionized water.
[0018] Its preparation method includes the preparation of slurry and the application process of hydrophobic mixture. The raw material components of the slurry are coniferous wood will and waste paper pulp, and other substances ...
Embodiment 3
[0020]A hydrophobic soft tissue paper, comprising the following raw materials in parts by weight: 66 parts of coniferous wood, 45 parts of waste paper pulp, 30 parts of synthetic wax, 4 parts of dehydroabietic acid, 4 parts of dihydroabietic acid, tetrahydroabietic acid 4 parts of acid, 15 parts of esterified rosin, 20 parts of modified fuma rosin, 17 parts of maleic acid resin, 7 parts of acetic acid, 10 parts of polyoxyethylene sorbitan tristearate, 1-mercaptododecane 4 parts, 16 parts of dimethylaminoethyl methacrylate, 14 parts of potassium persulfate, 19 parts of cetyltrimethylammonium halide, 13 parts of acrylamide, 17 parts of stearic acid, 13 parts of edible alkali, borax 7 parts, 100 parts of deionized water
[0021] Its preparation method includes the preparation of slurry and the application process of hydrophobic mixture. The raw material components of the slurry are coniferous wood will and waste paper pulp, and other substances are all hydrophobic mixtures. The a...
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com