[0029] This environmentally friendly extreme pressure metalworking concentrate is prepared by:
[0030] Step 1: Add 1.5 parts of paraffin wax, 0.8 parts of fatty alcohol, 0.4 parts of organic ester, 0.3 parts of hexanediol and 8 parts of tap water into the mixing tank, mix and stir evenly, and take them out into the container to obtain polyether modified silicone Type defoamer to clean the mixing tank;
[0031] Step 2: uniformly mixing 4 parts of nonylphenol polyoxyethylene ether and 2 parts of lauryl alcohol polyoxyethylene ether to obtain a surfactant;
[0032] Step 3: Put 100 parts of base oil, 60 parts of oily agent, 80 parts of pentaerythritol oleate and 40 parts of isosteric stearyl alcohol into a mixing tank, mix and stir evenly to obtain mixed solution 1, take out mixed solution 1, and stir the tank is cleaned;
[0033] Step 4: Mix and stir 60 parts of pH value adjusting agent, 12 parts of organic corrosion inhibitor, 70 parts of rust inhibitor and 75 parts of pure w...
Embodiment 2
[0038] This environmentally friendly extreme pressure metalworking concentrate is prepared by:
[0039] Step 1: Add 1.8 parts of paraffin wax, 1 part of fatty alcohol, 0.3 parts of organic ester, 0.4 part of hexanediol and 7 parts of tap water into the mixing tank, mix and stir evenly, and take them out into the container to obtain polyether modified silicone Type defoamer to clean the mixing tank;
[0040] Step 2: uniformly mix 5 parts of nonylphenol polyoxyethylene ether and 3 parts of lauryl alcohol polyoxyethylene ether to obtain a surfactant;
[0041] Step 3: Put 130 parts of base oil, 85 parts of oiliness agent, 60 parts of pentaerythritol oleate and 50 parts of isomeric stearyl alcohol into a mixing tank, mix and stir evenly to obtain mixed solution 1, take out mixed solution 1, and stir the tank is cleaned;
[0042] Step 4: Mix and stir 80 parts of pH value adjusting agent, 18 parts of organic corrosion inhibitor, 95 parts of rust inhibitor and 95 parts of pure water...
Embodiment 3
[0047] This environmentally friendly extreme pressure metalworking concentrate is prepared by:
[0048] Step 1: Add 2 parts of paraffin wax, 0.5 part of fatty alcohol, 0.2 part of organic ester, 0.3 part of hexanediol and 10 parts of tap water into the mixing tank, mix and stir evenly, and take it out and put it into the container to obtain polyether modified silicone Type defoamer to clean the mixing tank;
[0049] Step 2: uniformly mixing 4 parts of nonylphenol polyoxyethylene ether and 3 parts of lauryl alcohol polyoxyethylene ether to obtain a surfactant;
[0050] Step 3: Put 120 parts of base oil, 85 parts of oily agent, 50 parts of pentaerythritol oleate and 30 parts of isomeric stearyl alcohol into a mixing tank, mix and stir evenly to obtain mixed solution 1, take out mixed solution 1, and stir the tank is cleaned;
[0051] Step 4: Mix and stir 70 parts of pH adjuster, 15 parts of organic corrosion inhibitor, 80 parts of rust inhibitor and 90 parts of pure water to o...