Embodiment 1
[0048] Add sodium carbonate decahydrate and circulating mother liquor to the slurry tank at a mass ratio of 2:1, heat up to 30-40°C to dissolve, then add sodium chloride, so that the mass content of sodium chloride in the slurry is 15%, and the obtained The first reaction solution: Add 5 g of ethylenediaminetetraacetic acid (EDTA) and 5 g of aminotrimethylene phosphonic acid (ATMP) into a hydrogen peroxide solution with a mass concentration of 50% per kilogram, stir and dissolve to make a hydrogen peroxide mixed solution, which is the second The reaction solution was cooled to 0-10°C for later use; 100 g of sodium pyrophosphate was added to every kilogram of water, stirred and dissolved to obtain the third reaction solution.
[0049] Add circulating mother liquid into the reaction kettle as the bottom liquid, control the reaction temperature at 18-30°C, and prepare the prepared sodium carbonate decahydrate slurry (first reaction liquid) at 3.41m 3 / h, hydrogen peroxide mixed s...
Embodiment 2
[0051] Add sodium carbonate decahydrate and circulating mother liquor to slurry tank 1 at a mass ratio of 2:1, heat up to 30-40°C to dissolve, then add sodium chloride, so that the mass content of sodium chloride in the slurry is 15-18% , to obtain a first-level first reaction solution; sodium carbonate decahydrate and circulating mother liquor are added to the slurry tank 2 with a mass ratio of 2:1, heated to 30-40 ° C for dissolution, and then sodium chloride is added to make the chlorination in the slurry The mass content of sodium is 26-30%, and the secondary first reaction solution is prepared; 0.5 g of sodium polyacrylate and 0.8 g of hydroxyethylene diphosphoric acid are added to the hydrogen peroxide solution with a mass concentration of 27.5% per kilogram, and stirred and dissolved to prepare The hydrogen peroxide mixed solution is used as the second reaction solution, cooled to 0-10°C for later use; 150 g of sodium tripolyphosphate is added to each kilogram of water, ...
Embodiment 3
[0054] Add sodium carbonate decahydrate and circulating mother liquor to No. 1 slurry tank at a mass ratio of 2:1, heat up to 30-40°C to dissolve, then add sodium chloride, so that the mass content of sodium chloride in the slurry is 15-18 %, to obtain a first-level first reaction solution; aqueous sodium carbonate and circulating mother liquor are added to the No. 2 slurry tank with a mass ratio of 2:1, the temperature is raised to 30-40 ° C for dissolving, and then sodium chloride is added to make the slurry in the slurry The mass content of sodium chloride is 18-26%, and the secondary first reaction solution is obtained; Sodium carbonate decahydrate and circulating mother liquor are added to No. 3 slurry tank with a mass ratio of 2:1, and the temperature is raised to 30-40°C for dissolution , add sodium chloride again, make the mass content of the sodium chloride in the slurry be 26-30%, make three-stage first reaction liquid; Add magnesium sulfate 0.2g, 0.5g of EDTA and 0....
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com