Energy-saving environment protection fire coal additive agent and method of manufacturing the same
A coal-fired additive, energy-saving and environment-friendly technology, applied in the field of resources and environment, can solve the problems of air pollution, insufficient combustion of raw coal, etc., and achieve the effects of complete combustion, increased flame height, and reduced carbon content in slag
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] The selected coal-fired additive composition and its mass ratio are as follows:
[0031] Potassium nitrate 28Kg; manganese dioxide 56Kg; potassium chlorate 54Kg; sodium nitrate 26Kg; ethylenediaminetetraacetic acid 40Kg; hexamethylenetetramine 18Kg; ammonium nitrate 30Kg; sodium carbonate 20Kg;
[0032] Select formula raw materials according to the above-mentioned energy-saving and environment-friendly coal-fired additives; grind the selected formula raw materials into powder through a grinder; mix the pulverized raw materials into 1000 parts of water, stir well, and leave for 24 hours to obtain the coal-fired additive stock solution.
Embodiment 2
[0034] The selected coal-fired additive composition and its mass ratio are as follows:
[0035] Potassium nitrate 28Kg; manganese dioxide 56Kg; potassium chlorate 54Kg; sodium nitrate 26Kg; ethylenediaminetetraacetic acid 40Kg; hexamethylenetetramine 18Kg; ammonium nitrate 30Kg; sodium carbonate 20Kg;
[0036] Potassium permanganate 34Kg can also be put into the above-mentioned coal combustion additive. Potassium permanganate is an oxidizing agent, which can be decomposed at different temperatures, so that coal can be fully burned at different temperatures.
[0037] Select formula raw materials according to the above-mentioned energy-saving and environment-friendly coal-fired additives; grind the selected formula raw materials into powder through a grinder; mix the pulverized raw materials into 1000 parts of water, stir well, and leave for 24 hours to obtain the coal-fired additive stock solution.
Embodiment 3
[0039] The selected coal-fired additive composition and its mass ratio are as follows:
[0040] Potassium nitrate 25Kg; manganese dioxide 60Kg; potassium chlorate 55Kg; sodium nitrate 25Kg; ethylenediaminetetraacetic acid 42Kg; hexamethylenetetramine 20Kg; ammonium nitrate 35Kg; sodium carbonate 25Kg;
[0041] Potassium permanganate 35Kg can also be put into the above-mentioned coal-fired additive composition.
[0042] Select formula raw materials according to the above-mentioned energy-saving and environment-friendly coal-fired additives; grind the selected formula raw materials into powder through a grinder; mix the pulverized raw materials into 1000 parts of water, stir well, and leave for 24 hours to obtain the coal-fired additive stock solution.
[0043] The stock solution of the coal-fired additive prepared according to the above method can be stored for 3 years without deterioration; the coal mixed with the coal-fired additive according to the above method can be stored...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com