Multi-component composite metal antirust paint and its preparation method

A metal anti-rust, multi-component technology, applied in the direction of anti-corrosion coatings, coatings, epoxy resin coatings, etc., can solve the problems of easy cracking or peeling of the paint film, endangering health, and increasing construction costs, etc., to achieve low cost , good adhesion, increase the effect of corrosion resistance and heat resistance

Active Publication Date: 2013-03-20
佛山市顺德区姿彩塑料粉末实业有限公司
View PDF5 Cites 8 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] In recent years, epoxy zinc-rich paint is the most commonly used industrial anti-rust paint to protect metal. Due to the relatively high density of metal zinc powder, in order not to To settle or slow down the settling speed of zinc powder, it is necessary to add a certain amount of anti-settling agent to the paint; the viscosity of the paint will also increase when the anti-settling agent is added. When selecting polyamide resin, it is necessary to choose as small a Molecular weight resin (E44); in order to meet the brushability during construction, a large amount of solvent should be added to the paint. During construction, the solvent seriously endangers the health of workers, and the solvent volatilizes into the air during the drying process to pollute the environment. The construction cost is increased; the brittleness of the paint film after the curing of the small molecular weight resin is large, and the thermal expansion and contraction of the metal is large, and the paint film is easy to crack or fall off when the temperature changes

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment

[0014] Example: Multi-component composite metal antirust paint, the weight parts of its raw materials are: polypropylene resin 34, bisphenol A epoxy resin 30, phenolic resin 12, modified sepiolite powder 22, 8-hydroxyquinoline 1.5, Dibutyl phthalate 22, calcium lignosulfonate 0.7, polybutylene terephthalate 0.6, poly-4-methyl-1-pentene 0.4, 4,4-methylenebis(2 , 6-di-tert-butylphenol) 1.2, modified styrene-acrylic emulsion 3.5, sodium hydroxymethylcellulose 1.6, vinyltrisilane 0.7, sodium stearate 0.6 and sodium dodecylbenzenesulfonate 1.2.

[0015] The preparation method of the multi-component composite metal antirust paint comprises the following steps:

[0016] (1) Mix and stir polypropylene resin, bisphenol A epoxy resin, phenolic resin, modified sepiolite powder, modified styrene-acrylic emulsion and dibutyl phthalate evenly according to the weight of the raw materials, and disperse at high speed And grind to a fineness below 35um;

[0017] (2) Add 8-hydroxyquinoline, c...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a multi-component composite metal antirust paint and its preparation method. The metal antirust paint is composed of the following raw materials, by weight, 32-35 parts of a polypropylene resin, 28-32 parts of a bisphenol A epoxy resin, 10-15 parts of a phenolic resin, 17-25 parts of modified meerschaum powder, 1.4-1.6 parts of 8-hydroxyquinoline, 20-25 parts of dibutyl phthalate, 0.6-0.8 parts of calcium lignin sulphonate, 0.4-0.8 parts of polybutylene terephthalate, 0.3-0.5 parts of poly-4-methyl-1-pentene, 1.1-1.3 parts of 4,4-methylene-bis(2,6-di-t-butylphenol), 2-5 parts of a modified styrene-acrylate emulsion, 1.5-1.7 parts of carboxymethyl cellulose sodium, 0.4-1.0 part of vinyltrisilane, 0.4-0.7 parts of sodium stearate and 1.0-1.5 parts of sodium dodecyl benzene sulfonate. The film of the metal antirust paint has the advantages of good adhesion, fast drying, good heat resistance, environmental protection and no pollution, and the modified meerschaum powder and the modified styrene-acrylate emulsion which are added to the raw materials improve the excellent performances of high-polymer materials in the raw materials and simultaneously increase the corrosion and heat resistances of the metal antirust paint; and the preparation method of the metal antirust paint has the advantages of simplicity, low cost and suitableness for large-scale production.

Description

technical field [0001] The invention relates to a multi-component composite metal antirust paint and a preparation method thereof, belonging to the technical field of antirust materials. Background technique [0002] In recent years, epoxy zinc-rich paint is the most used industrial anti-rust paint to protect metal. Due to the relatively high density of metal zinc powder, in order to prevent the zinc powder from settling or slow down the settling speed of the zinc powder, it is necessary to add A certain amount of anti-settling agent; the viscosity of the paint will also increase when the anti-settling agent is added. When selecting polyamide resin, it is necessary to choose a resin with a small molecular weight (E44) as much as possible; in order to meet the brushability during construction , to add a large amount of solvent to the paint, the solvent seriously endangers the health of workers during construction, the solvent volatilizes into the air during the drying proces...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C09D133/12C09D163/02C09D161/06C09D125/14C09D5/08
Inventor 肖颖张蔓青
Owner 佛山市顺德区姿彩塑料粉末实业有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products