Method for preparing coating carrying growth factor on surface of bone injury repair material

A bone injury repair and growth factor technology, applied in coatings, medical science, prostheses, etc., can solve the problems of poor effect, low stability, and short osteoinductive action time, and achieve good stability and osteoinductive effect Good, long-lasting osteoinductive effect

Inactive Publication Date: 2013-07-10
SOUTHWEST JIAOTONG UNIV
View PDF3 Cites 15 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Generally, the construction of polyelectrolyte multilayer films relies on the alternating deposition of positive and negative charges, and the molecular layers are assembled by electrostatic adsorption. This non-crosslinked self-assembled film will lead to the deposition of polyelectrolytes, which are originally weak in electricity, on the surface of the material. Insufficient strength, the membrane unit layer is easy to degrade and interdiffused in the biological environment, and the stability is not high. On the other hand, growth factors and other biologically active molecules are assembled between the membrane layers through their own electricity and the polyelectrolyte layer through electrostatic interaction Or directly chemically grafted with the self-assembled membrane, which also enables the rapid release of these biomolecules with the degradation of the polyelectrolyte membrane
Therefore, the osteoinductive action time of biomolecules is short and the effect is poor

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0026] A method for preparing a growth factor-loaded coating on the surface of a bone damage repairing material, comprising the steps of:

[0027] A, the growth factor---bone morphogenetic protein (BMP) is dissolved in the chondroitin sulfate solution that concentration is 1mg / ml, obtains the mixed solution that bone morphogenetic protein concentration is 0.5 μ g / ml, mixes mixed solution and concentration again 1 mg / ml chitosan solution was mixed at a volume ratio of 1:2, stirred, centrifuged, freeze-dried, and then dissolved in water to prepare positively charged bone-loaded morphogenetic protein micro-nanospheres with a concentration of 1 mg / ml solution;

[0028] B. The sodium alginate which is negatively charged in the solution and contains o-diol is formulated into a solution with a concentration of 20 mg / ml, and the solution is mixed with an equal volume of sodium periodate aqueous solution and stirred for 6 hours under light-proof conditions. Wherein the molar ratio of ...

Embodiment 2

[0037] A method for preparing a growth factor-loaded coating on the surface of a bone damage repairing material, comprising the steps of:

[0038] A. Dissolving the growth factor——vascular endothelial growth factor (VEGF) in the heparin solution with a concentration of 2 mg / ml to obtain a mixed solution with a concentration of vascular endothelial growth factor of 10 μg / ml, and then mixing the mixed solution with a concentration of 3 mg / ml The polylysine solution was mixed at a volume ratio of 1:10, stirred, centrifuged, freeze-dried, and then dissolved in water to prepare a solution of positively charged micro-nanospheres loaded with vascular endothelial growth factor at a concentration of 0.5 mg / ml ;

[0039]B. The negatively charged hyaluronic acid containing o-diol in the solution is prepared into a solution with a concentration of 20 mg / ml, and the solution is mixed with an equal volume of sodium periodate aqueous solution and stirred for 6 hours under light-proof conditi...

Embodiment 3

[0048] A method for preparing a growth factor-loaded coating on the surface of a bone damage repairing material, comprising the steps of:

[0049] A. Dissolving the growth factor—bone morphogenetic protein (BMP) in a sodium alginate solution with a concentration of 3 mg / ml to obtain a mixed solution with a bone morphogenetic protein concentration of 0.7 μg / ml, and then mixing the mixed solution with a concentration of The polylysine solution of 2 mg / ml was mixed according to the volume ratio of 1:6, stirred, centrifuged, freeze-dried, and then dissolved in water to prepare the micronano ball solution;

[0050] B. The chondroitin sulfate, which is negatively charged in the solution and contains vicinal diol, is formulated into a solution with a concentration of 20 mg / ml, and the solution is mixed with an equal volume of sodium periodate aqueous solution and stirred for 6 hours under light-proof conditions. Wherein the molar ratio of sodium periodate and chondroitin sulfate mon...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
concentrationaaaaaaaaaa
Login to View More

Abstract

The invention discloses a method for preparing a coating carrying out a growth factor on the surface of a bone injury repair material. According to the method, 5 to 100 unit films are formed on the surface of the material through a layer-by-layer self-assembly process; four layers of unit films comprise a polyelectrolyte layer (polycation layer with amino) with positive charges, a polysaccharide oxide layer (with negative charges), a growth factor embedding micro and nano particle layer with positive charges and a polysaccharide oxide layer (with negative charges) from inside to outside. Micro and nano particles with negative charges in the unit films are sandwiched between the two polysaccharide oxide layers with the negative charges through electrostatic adsorption, and the amino carried by the micro and nano particles can be covalently bound with the aldehyde group of polysaccharide oxides, so that the micro and nano particles are well immobilized in the unit films. The unit films can be covalently bound and crosslinked with each other through the polycation with the amino and the polysaccharide oxide with the aldehyde group, achieve an electrostatic adsorption effect due to opposite electric properties, and have strong binding force; and the coating is high in stability, slow in degradation, long and controllable in bone induction acting time and good in bone induction effect.

Description

technical field [0001] The invention relates to a method for preparing a growth factor-loaded coating on the surface of a bone damage repairing material. Background technique [0002] Due to their good mechanical properties and biocompatibility, metal medical material alloys are often used as bone repair materials, that is, bone tissue replacement materials, to be implanted in the human body. After implanted into the human body, the interaction between bone repair materials and the surrounding environment in the body first occurs on the surface, and metal materials are biologically inert materials, so it is very important to modify the surface of the implant. In recent years, the method of modifying the surface of bone repair materials has been widely used clinically, especially the method of immobilizing growth factors on the surface of the material to endow the material with osteoinductivity has been extensively studied. [0003] The surface of the material builds a polye...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): A61L27/54A61L27/34A61L27/40A61L27/28
Inventor 鲁雄董丽王振铭谢超鸣韩璐刘敏
Owner SOUTHWEST JIAOTONG UNIV
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products