A technology of waterproof paint and starch, which is applied in the field of decorative materials, can solve the problems of being uneconomical, practical, popular, not suitable for large-scale industrial production, and the waterproof effect of waterproof paint is not durable, etc., and achieve superior UV aging resistance and water resistance Anti-contamination ability, low cost effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] A decorative waterproof paint, comprising the following raw materials in parts by weight: 26 parts of epoxy resin, 17 parts of butyl p-hydroxybenzoate, 18 parts of carboxymethyl cellulose, 15 parts of white latex, 8 parts of ethylenediamine, nano 11 parts of silicon dioxide, 18 parts of talc, 16 parts of castor oil, 12 parts of polyether polyol, 19 parts of modified starch, 11 parts of thinner, 5 parts of polyurethane film former, 8 parts of binder and 17 parts of water .
[0031] A preparation method for decorative waterproof paint, comprising the following preparation steps:
[0032] a. Mix epoxy resin and butyl p-hydroxybenzoate, introduce into the reaction kettle, heat up to 75°C, stir and react for 0.8h, and obtain mixture 1;
[0033]b. Mix nano-silica, talcum powder, ethylenediamine and water, introduce it into the stirring tank, stir continuously and raise the temperature to 58°C, then add polyether polyol dropwise, and stir at a speed of 900r / min until the addi...
Embodiment 2
[0041] A decorative waterproof paint, comprising the following raw materials in parts by weight: 23 parts of epoxy resin, 12 parts of butyl p-hydroxybenzoate, 15 parts of carboxymethyl cellulose, 15 parts of white latex, 13 parts of ethylenediamine, nano 17 parts of silicon dioxide, 17 parts of talcum powder, 16 parts of castor oil, 8 parts of polyether polyol, 19 parts of modified starch, 7 parts of thinner, 5 parts of polyurethane film former, 13 parts of binder and 17 parts of water .
[0042] A preparation method for decorative waterproof paint, comprising the following preparation steps:
[0043] a. Mix epoxy resin and butyl p-hydroxybenzoate, introduce into the reaction kettle, heat up to 75°C, stir and react for 0.7h, and obtain mixture 1;
[0044] b. Mix nano-silica, talcum powder, ethylenediamine and water, introduce it into the stirring tank, stir continuously and raise the temperature to 58°C, then add polyether polyol dropwise, and stir at a speed of 900r / min unti...
Embodiment 3
[0052] A decorative waterproof paint, comprising the following raw materials in parts by weight: 25 parts of epoxy resin, 15 parts of butyl p-hydroxybenzoate, 17 parts of carboxymethyl cellulose, 15 parts of white latex, 9 parts of ethylenediamine, nano 17 parts of silicon dioxide, 16 parts of talc, 12 parts of castor oil, 10 parts of polyether polyol, 16 parts of modified starch, 10 parts of thinner, 5 parts of polyurethane film former, 11 parts of binder and 15 parts of water .
[0053] A preparation method for decorative waterproof paint, comprising the following preparation steps:
[0054] a. Mix epoxy resin and butyl p-hydroxybenzoate, introduce into the reaction kettle, heat up to 78°C, stir and react for 0.8h, and obtain mixture 1;
[0055] b. Mix nano-silica, talc powder, ethylenediamine and water, introduce it into the stirring tank, stir continuously and raise the temperature to 58°C, then add polyether polyol dropwise, and stir at a speed of 800r / min until the addi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com