Deodorant for papermaking industry and preparation method thereof
A deodorant and papermaking technology, applied in the field of papermaking, can solve the problems of poor deodorization effect and increase the production cost of manufacturers, achieve good deodorization effect, reduce production cost, and have broad application prospects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] A paper-making deodorant, comprising the following raw materials in parts by weight: 35 kilograms of ferrous sulfate, 22 kilograms of ammonium persulfate, 25 kilograms of ammonium sulfite, 2.4 kilograms of zinc chloride, 0.4 kilograms of sodium tripolyphosphate, Cellulose 0.6 kg and magnesium sulfate 2.8 kg.
[0024] The preparation method of described papermaking deodorant, concrete steps are as follows:
[0025] Step 1, taking raw materials according to the proportion;
[0026] Step 2, mixing ferrous sulfate, ammonium persulfate, ammonium sulfite, zinc chloride and magnesium sulfate in a dry mixing tank and stirring for 52 minutes to obtain the first mixture;
[0027] Step 3, adding sodium tripolyphosphate and methyl cellulose to the first mixture and stirring at a speed of 540rpm for 23 minutes to obtain a second mixture;
[0028] Step 4, the second mixture was left to stand for 36 minutes and packed in a plastic barrel with a plastic film to obtain the finished pr...
Embodiment 2
[0030] A paper-making deodorant, comprising the following raw materials in parts by weight: 38 kilograms of ferrous sulfate, 23.6 kilograms of ammonium persulfate, 26 kilograms of ammonium sulfite, 2.7 kilograms of zinc chloride, 0.45 kilograms of sodium tripolyphosphate, Cellulose 0.72 kg and magnesium sulfate 3.4 kg.
[0031] The preparation method of described papermaking deodorant, concrete steps are as follows:
[0032] Step 1, taking raw materials according to the proportion;
[0033] Step 2, mixing ferrous sulfate, ammonium persulfate, ammonium sulfite, zinc chloride and magnesium sulfate at 24 degrees Celsius and stirring at a speed of 660 rpm for 65 minutes to obtain the first mixture;
[0034] Step 3, adding sodium tripolyphosphate and methyl cellulose to the first mixture and stirring at a speed of 450rpm for 18 minutes to obtain a second mixture;
[0035] Step 4, the second mixture was left to stand for 33 minutes and packaged to obtain the finished product.
Embodiment 3
[0037] A paper-making deodorant, comprising the following raw materials in parts by weight: 40 kg of ferrous sulfate, 25 kg of ammonium persulfate, 26.7 kg of ammonium sulfite, 3 kg of zinc chloride, 0.5 kg of sodium tripolyphosphate, Cellulose 0.8 kg and magnesium sulfate 4 kg.
[0038] The preparation method of described papermaking deodorant, concrete steps are as follows:
[0039] Step 1, taking raw materials according to the proportion;
[0040] Step 2, mixing ferrous sulfate, ammonium persulfate, ammonium sulfite, zinc chloride and magnesium sulfate in a dry mixing tank at 25 degrees Celsius and stirring at a speed of 540 rpm for 60 minutes to obtain the first mixture;
[0041] Step 3, adding sodium tripolyphosphate and methyl cellulose to the first mixture and continuing stirring at a speed of 720rpm for 20 minutes to obtain a second mixture;
[0042] Step 4, the second mixture was left to stand for 30 minutes and packed in a plastic barrel with a plastic film to obta...