The invention belongs to the technical field of rubber, and specifically discloses an anti-aging rubber, which is prepared from the following components in parts by weight: 70-90 parts of natural rubber SVR3L, 10-30 parts of butadiene rubber 9000, 5-8 parts of zinc oxide, 1-2 parts of stearic acid, 5-8 parts of ordinary paraffin, 3-5 parts of microcrystalline wax, 3-5 parts of coumarone resin, 2-3 parts of coupling agent, 2-5 parts of dispersing aid, softener 5-10 parts, anti-aging agent mixture 5-7 parts, accelerator mixture 1.3-1.8 parts, carbon black mixture 70-85 parts, sulfur 1.8-2.5 parts, anti-scorch agent 0.2-0.4 parts. The anti-aging agent mixture is anti-aging agent RD, anti-aging agent 4010NA, and the accelerator mixture is accelerator CZ, accelerator DM, and accelerator TMTD. The anti-aging rubber of the invention has good anti-oxidation and anti-aging capabilities, and good mechanical strength and fatigue resistance.