High-strength building wallboard
A high-strength and architectural technology, applied in the direction of building materials, can solve the problems of low strength, high production cost, and use, and achieve the effect of improving mechanical properties, high strength, and avoiding degradation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] 1. Modified nylon: Dry nylon 6 and lithium chloride in an oven until the water content is below 0.1%, ball-mill lithium chloride in a ball mill, and pass through a 100-mesh sieve. The parts by weight of the following components are: Nylon 6: 95 parts; Lithium chloride: 5 parts. The two were mixed in an internal mixer for 5 minutes, and the temperature was set at 240 ° C. After mixing, the low melting point nylon 6 was crushed in the crusher.
[0024] 2. Wood-plastic preparation: The weight fractions of the following components are: low melting point nylon 6:50 parts, wood fiber: 40 parts, isocyanate chain extender: 5 parts, stearic acid: 3 parts, iron oxide red: 2 parts . The above materials are mixed in a mixer and granulated by a granulator, and the granulated material is extruded into shape.
Embodiment 2
[0026] 1. Modified nylon: Dry nylon 66 and calcium chloride in an oven until the water content is below 0.1%. After ball milling calcium chloride in a ball mill, pass through a 100-mesh screen. The parts by weight of the following components are respectively Nylon 66: 85 parts; Lithium chloride: 15 parts. Mix the two in an internal mixer for 6 minutes, set the temperature at 260°C, and crush the low-melting nylon 66 after mixing in a crusher.
[0027] 2. Wood-plastic preparation: the weight fractions of the following components are: low melting point nylon 66:80 parts, wood fiber: 15 parts, zinc stearate: 3 parts, iron oxide yellow: 2 parts. The above materials are mixed in a mixer and granulated by a granulator, and the granulated material is injection molded.
Embodiment 3
[0029] 1. Modified nylon: Dry nylon 6 and lithium chloride in an oven until the moisture content is below 0.1%, mill lithium chloride in a ball mill, and pass through a 80-mesh screen. The parts by weight of the following components are respectively: Nylon 6: 97 parts; Lithium chloride: 3 parts, the two are mixed in a mixer, and then granulated, and the temperature of each zone is set as follows:
[0030] interval
[0031] 2. Wood-plastic preparation: The weight fractions of the following components are: low melting point nylon 6:30 parts, wood fiber: 60 parts, epoxy resin chain extender: 5 parts, zinc stearate: 3 parts, iron oxide yellow : 2 servings. The above materials are mixed in a mixer and granulated by a granulator, and the granulated material is extruded into shape.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com