A technology of power cable and sheath layer, applied in the field of waterproof power cable, can solve the problems of insulation resistance and breakdown voltage drop, easy to breed bacteria to corrode the sheath layer, unable to find the positioning in time, etc. Enhanced toughness and moderate hardness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A kind of waterproof power cable proposed by the present invention comprises a conductor and a sheath layer coated on the outside of the conductor; the raw materials of the sheath layer include by weight: 25 parts of chlorinated rubber, 42 parts of EPDM rubber, and 0.5 part of sulfur , 0.6 parts of stearic acid, 0.1 parts of triallyl isocyanurate, 3 parts of magnesium oxide, 15 parts of modified kaolin, 28 parts of sepiolite powder, 40 parts of white carbon black, 8 parts of heavy calcium carbonate, 11 parts of halloysite, 9 parts of glass fiber, 0.5 part of chlorinated paraffin, 2 parts of pentaerythritol ester, 0.2 part of anti-aging agent RD, and 2 parts of anti-aging agent D.
Embodiment 2
[0018] A waterproof power cable proposed by the present invention includes a conductor and a sheath layer coated on the outside of the conductor; the raw materials of the sheath layer include by weight: 35 parts of chlorinated rubber, 30 parts of EPDM rubber, and 1.2 parts of sulfur , 0.1 part of stearic acid, 0.6 part of triallyl isocyanurate, 1 part of magnesium oxide, 25 parts of modified kaolin, 20 parts of sepiolite powder, 60 parts of white carbon black, 2 parts of heavy calcium carbonate, 15 parts of halloysite, 4 parts of glass fiber, 1.5 parts of chlorinated paraffin, 1 part of pentaerythritol ester, 0.8 part of anti-aging agent RD, and 1 part of anti-aging agent D.
[0019] The modified kaolin in the raw material of the sheath layer is prepared by the following process: mix and stir lauryl amidopropyl betaine and water, add copper sulfate solution dropwise, stir after the addition is complete, and use sodium hydroxide to adjust the pH of the system to 8.5-9.2 , then ...
Embodiment 3
[0021] A kind of waterproof power cable proposed by the present invention comprises a conductor and a sheath layer coated on the outside of the conductor; the raw materials of the sheath layer include by weight: 28 parts of chlorinated rubber, 38 parts of EPDM rubber, and 0.8 part of sulfur , 0.5 parts of stearic acid, 0.3 parts of triallyl isocyanurate, 2.5 parts of magnesium oxide, 18 parts of modified kaolin, 26 parts of sepiolite powder, 45 parts of white carbon black, 6 parts of heavy calcium carbonate, 12 parts of halloysite, 7 parts of glass fiber, 0.8 parts of chlorinated paraffin, 1.8 parts of pentaerythritol ester, 0.4 parts of anti-aging agent RD, and 1.7 parts of anti-aging agent D.
[0022] The modified kaolin in the raw material of the sheath layer is prepared by the following process: 3 parts by weight of lauryl amidopropyl betaine and 40 parts of water are mixed and stirred, and 2.5 parts of copper sulfate solution with a concentration of 4.5wt% is added dropwis...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com