[0018] A kind of paint defoamer, in parts by mass, adopts following steps to make:
[0019] S1, mix 20 parts of polydimethylsiloxane, 8 parts of high carbon alcohol, 3 parts of fumed white carbon black, 5 parts of tributyl phosphate, 2 parts of distearamide, and 0.5 parts of potassium hydrogen persulfate Finally, stir evenly to obtain liquid A;
[0020] S2, add 3 parts of sodium hexametaphosphate, 2 parts of sorbitan fatty acid and 3 parts of carboxymethyl cellulose into 85 parts of deionized water, and stir evenly to obtain liquid B;
[0021] S3, mix liquid A and liquid B at 70°C, heat up to 100°C and stir evenly, then add 15 parts of hydrophobic silicon dioxide and keep warm for 30 minutes to prepare a paint defoamer.
Embodiment 2
[0023] A kind of paint defoamer, in parts by mass, adopts following steps to make:
[0024] S1, 30 parts of polymethyltriethoxysilane, 5 parts of higher carbon alcohol, 1 part of fumed white carbon black, 8 parts of tributyl phosphate, 0.5 parts of distearyl diethylamine, and 2 parts of potassium hydrogen persulfate After mixing, stir evenly to obtain liquid A;
[0025] S2, add 3 parts of sodium hexametaphosphate, 5 parts of polysorbate and 1.5 parts of carboxyethyl cellulose into 70 parts of deionized water, and stir evenly to prepare liquid B;
[0026] S3, Mix liquid A and liquid B at 60°C, heat up to 90°C and stir evenly, then add 30 parts of hydrophobic silicon dioxide and 3 parts of diethylene glycol laurate, and keep warm for 40 minutes to prepare a paint defoamer .
Embodiment 3
[0028] A kind of paint defoamer, in parts by mass, adopts following steps to make:
[0029] S1, mix 40 parts of polymethyltrimethoxysilane, 15 parts of higher carbon alcohol, 2 parts of fumed white carbon black, 6 parts of tributyl phosphate, 1 part of distearyl diethylamine, and 1 part of potassium hydrogen persulfate Finally, stir evenly to obtain liquid A;
[0030] S2, add 2 parts of sodium hexametaphosphate, 3 parts of fatty acid esters of glycerol and 2 parts of xanthan gum into 75 parts of deionized water, and stir evenly to prepare liquid B;
[0031] S3, mix liquid A and liquid B at 65°C, heat up to 95°C and stir evenly, then add 20 parts of hydrophobic silicon dioxide, 2 parts of diethylene glycol laurate and 2 parts of glutaraldehyde, and keep warm for 35 minutes. Prepared paint defoamer.
PUM

Abstract
Description
Claims
Application Information

- Generate Ideas
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com