Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Preparation of organosilicon-modified vinyl ester resin: In parts by weight, add 83 parts of cyclohexanone and 12 parts of n-butanol into a reaction kettle equipped with a thermometer and a stirrer, start the stirrer, and heat in a water bath To 50°C, add 1 part of sodium acrylamido isopropyl sulfonate, after it is completely dissolved, add 0.4 part of sodium 1-propenyl-2-hydroxyalkane sulfonate, 0.8 part of tetraisopropyl titanate, naphthenic acid 0.3 part of bismuth, 56 parts of bisphenol A epoxy resin, slowly add 30 parts of aminopropyltrimethoxysilane dropwise after 8 minutes of heat preservation, after the dropwise addition, stir and react for 2 hours, and then spin evaporate to remove cyclohexanone and n-butanol to obtain Silicone-modified epoxy resin, then add 0.5 parts of N, N-dimethylaniline, 36 parts of methacrylic acid, under nitrogen atmosphere, heat up to 95°C and stir for 1 hour, then continue to heat up to 120°C, continue to stir for 2 hours, and react Th...
Embodiment 2
[0021] Preparation of polyurethane-modified vinyl ester resin: vacuum dehydrate the polymer polyol at 125°C for 1 hour; add diisocyanate, stir for 1 hour at a temperature of 80°C and a vacuum pressure of -0.06MPa; add a catalyst, React for 1h at a temperature of 85°C and a reaction pressure of 0.03MPa; add a polymerization inhibitor and vinyl ester resin, stir for 2h at a temperature of 60°C and a reaction pressure of 0.08MPa, and analyze the NCO group with an infrared spectrometer Content, when the peak of NCO disappears completely, stop heating reaction, obtain polyurethane modified vinyl ester resin; The mol ratio of polymer polyol, diisocyanate and vinyl ester resin in described polyurethane modified vinyl ester resin is: 1:1.4:1, the catalyst and the polymerization inhibitor each account for 0.1‰ of the weight of the polyurethane modified vinyl ester resin; the polymer polyol includes polyether ester diol and polystyrene polyol in a mass ratio of 1:1 The first step of the...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com