Sweat-removing antibacterial and skin-friendly fabric and preparation method thereof
An antibacterial fabric and fabric technology, which is applied in the manufacture of rayon, fabric surface trimming, textile material processing, etc., can solve the problems of poor use strength, easy breakage, wear, etc. The effect of durability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0023] Fabric is a textile raw material commonly used in daily necessities. It is used in daily necessities, food, housing and transportation, and there are many kinds of fabrics, such as cotton cloth, linen cloth, silk, woolen cloth, chemical fiber, blended spinning, etc. People choose different fabric materials to sew according to different needs in daily use. However, for the practicability of the fabric, most of them hope that the fabric has high strength, wear resistance and antibacterial effect to ensure the durability of use. However, the existing fabrics have the problems of poor strength in use and easy damage and wear. In order to solve the above technical problems, the present invention proposes a preparation method of perspiration antibacterial skin-friendly fabric, which is characterized in that it comprises the following steps: weighing each component according to the following parts by weight: 25-40 parts of modified soybean protein fiber , 10-15 parts of cotton...
Embodiment 1
[0036] Weigh graphite powder, sodium nitrate, strong oxidizing agent, potassium permanganate, hydrogen peroxide according to the weight ratio of 1:1:10:2:5, add strong oxidizing agent into the container, then add graphite powder and sodium nitrate and stir for 0.5h; Add potassium permanganate to the container again, the reaction temperature is 15°C, stir for 0.5h; heat up to 30°C and stir for 1h; add purified water and hydrogen peroxide and heat up to 85°C, stir for 0.5h, then carry out the solution in the container Filtrating, washing, drying, and pulverizing to obtain modified graphene oxide;
[0037] Weigh the bamboo fiber spinning liquid and modified graphene oxide according to the weight ratio of 1:0.05, pour the modified graphene oxide into the mixing tank containing alcohol organic solvent, and pour sulfuric acid into the mixing tank to adjust the pH When the value reaches 4, the bamboo fiber spinning solution is poured into the mixing tank and stirred for 0.5h, and the...
Embodiment 2
[0042] Weigh graphite powder, sodium nitrate, strong oxidizing agent, potassium permanganate and hydrogen peroxide according to the weight ratio of 1:2:15:5:8, add strong oxidizing agent into the container, then add graphite powder and sodium nitrate and stir for 1 hour; then Add potassium permanganate to the container, the reaction temperature is 25°C, stir for 1 hour; heat up to 40°C and stir for 2 hours; add purified water and hydrogen peroxide and heat up to 100°C, stir for 1 hour, then filter and wash the solution in the container , drying and crushing to obtain modified graphene oxide;
[0043] Weigh the bamboo fiber spinning liquid and modified graphene oxide according to the weight ratio of 1:0.2, pour the modified graphene oxide into the mixing tank containing ether organic solvent, and pour hydrochloric acid into the mixing tank to adjust the pH When the value reaches 5, the bamboo fiber spinning solution is poured into the mixing tank and stirred for 1 hour, and the...
PUM
Login to View More Abstract