Dry powder paint for construction as well as preparation method and use method thereof
A dry powder coating and construction technology, applied in powder coatings, coatings, etc., can solve the problems of less high-performance dry powder coatings and single products, and achieve the effect of convenient transportation and stable storage.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Example Embodiment
[0054] Example 1
[0055] In a newly-built residential area, in order to move in immediately after completion, the head of the household requires that there is no peculiar smell similar to that released by traditional latex paint, and the product of the present invention is used for interior wall decoration. The formula is (total weight is 100 kg): 30 kg redispersible ethylene-vinyl acetate copolymer (EVA) binary copolymer latex powder, 40 kg titanium dioxide, 10 kg calcium carbonate, 8.1 kg calcined kaolin, and talc 10 kg, 0.5 kg methyl cellulose ether, 0.2 kg solid defoamer, 0.8 kg solid dispersant, 0.3 kg solid thixotropic agent, 0.1 kg iron oxide red. When mixing, pour clean water into the mixer, the amount is 2.5 times of the dry powder paint, stir for 15 minutes, then let it stand for 12 minutes, and then stir for 3 minutes before use. The dry powder paint after mixing with water is applied by roller coating on the surface after the putty is made and leveled. Before rolle...
Example Embodiment
[0056] Example 2
[0057] The old wall inside the conference room of a company was renovated. The formula is (total weight is 100 kg): 15 kg redispersible vinyl acetate / ethylene / vinyl versatate terpolymer latex powder, 33 kg titanium dioxide, 38 kg calcium carbonate, 8 kg talc, methyl 0.1 kg of cellulose ether, 0.3 kg of solid defoamer, 0.4 kg of solid dispersant, and 0.2 kg of solid thixotropic agent. When mixing, pour clean water into the mixer, the amount is 3 times of the dry powder paint, stir for 15 minutes, then let it stand for 10 minutes, and then stir for 2 minutes before use. Because it has not been modified for many years, the walls collect a lot of dust and part of the wall falls off. The old wall was cleaned first, dust, floating layer and alkali layer were removed, and then putty was used to repair the wall. The putty was scraped on the 5th day after the repair, and smoothed with sandpaper after the initial drying, and the dry powder paint of the present inventi...
Example Embodiment
[0058] Example 3
[0059] In order to establish a high-end and environmentally-friendly shopping mall concept, the sales hall of a newly-built real estate was delivered as soon as possible and decorated with this dry powder coating. The formula is (total weight is 100 kg): 50 kg redispersible styrene-acrylate copolymer latex powder, 28.3 kg calcium carbonate, 10 kg calcined kaolin, 0.3 kg methyl cellulose ether, and 0.6 kg solid defoamer , 0.2 kg of solid dispersant, 0.6 kg of solid thixotropic agent, 10 kg of iron oxide red. When mixing, pour clean water into the agitator, the amount is twice that of the dry powder paint, stir for 15 minutes, then let it stand for 10 minutes, and then stir for 2 minutes before use. The spraying method is used for construction, and the painted wall is smooth, smooth and colorful, odorless, and pollution-free. It will start business the next day after the decoration is completed.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap