A technology for interior wall latex paint and cyanine powder, which is applied to the field of interior wall latex paint, can solve the problems of impact on scrub resistance, damage to the physical properties of the coating, and the effect is not optimal, so as to improve safety and environmental protection performance, good adhesiveness, Overcome flammable hazards and the effect of toxic active ingredients
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Example Embodiment
[0014] Example 1
[0015] Weigh the raw materials (kg) according to the following weight: Sesbania powder 5~7, Trimethylamine 0.6~0.9, Bamboo carbon powder 1~2, Photocatalyst 0.2~0.4, Acrylic acid emulsion 12~18, Hydroxyethyl cellulose thickener 0.2~0.6, wetting and dispersing agent 0.1~0.3, defoaming agent 0.1~0.3, film forming aid 0.6~0.9, titanium dioxide 6~10, heavy calcium 15~20, calcined kaolin 4~9, talc 4~10 , Preservative 0.15~0.35, Antifungal agent 0.15~0.35; and measure 160~170L water.
[0016] Preparation:
[0017] Add water to the stirred tank first, slowly add sesame powder under stirring, stir and infiltrate, and then add trimethylamine, hydroxyethyl cellulose thickener, wetting and dispersing agent, defoamer, and film-forming auxiliary in order; Add titanium dioxide, heavy calcium, bamboo carbon powder, photocatalyst, calcined kaolin, and talc; add vinegar-acrylic emulsion, preservative, and antifungal agent after turning to low speed and stir evenly; heat to 85°C an...
Example Embodiment
[0021] Further, preferred embodiment 2
[0022] Weigh the raw materials (kg) according to the following weight: Sesbania powder 6, Trimethylamine 0.8, Bamboo carbon powder 1.5, Photocatalyst 0.3, Acrylic acid emulsion 15, Hydroxyethyl cellulose thickener 0.4, Wetting and dispersing agent 0.15, Defoaming Agent 0.2, film-forming aid 0.7, titanium dioxide 8, heavy calcium 17, calcined kaolin 5, talc 7, preservative 0.2, antifungal agent 0.2; and measure 170L of water.
[0023] Preparation:
[0024] Add water to the stirred tank first, slowly add sesame powder under stirring, stir and infiltrate, and then add trimethylamine, hydroxyethyl cellulose thickener, wetting and dispersing agent, defoamer, and film-forming auxiliary in order; Add titanium dioxide, heavy calcium, bamboo carbon powder, photocatalyst, calcined kaolin, and talc; add vinegar-acrylic emulsion, preservative, and antifungal agent after turning to low speed and stir evenly; heat to 85°C and stir for 180 minutes at a con...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap