Method for preparing methane and barbecue charcoal from rhizoma curcumae dregs
A technology for grilling charcoal and medicinal residues, which can be applied to solid fuels, biofuels, waste fuels, etc., can solve problems such as pollution, waste of resources and environment, and reduce production costs, and achieve the effects of reducing environmental pollution, saving resources, and reducing production costs.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0059] The preparation method of described pyrolysis catalyst comprises the following steps:
[0060] S71: Mix alkaline clay, cobalt oxide, nickel oxide, titanium oxide, aluminum oxide, zinc oxide, and water glass for 8-12 minutes at a stirring speed of 100-160 r / min to prepare spherical particles I;
[0061] The preparation method of alkaline clay described in step S71, comprises the following steps:
[0062] S711: Mix bentonite and activated clay wastewater with a concentration of 10% in a weight ratio of 2:9, and stir evenly at a speed of 300 r / min to obtain slurry material I;
[0063] S712: Add the slurry material I prepared in step S711 to the inorganic mixed acid with a concentration of 16%, the inorganic mixed acid is phosphoric acid with a concentration of 19wt%, hydrochloric acid with a concentration of 38wt%, and sulfuric acid with a concentration of 27wt% by volume Mixed acid composed of 3:3:2, the weight ratio of slurry material I to inorganic mixed acid is 2:10, ...
Embodiment 1
[0081] A method for preparing methane and barbecue charcoal from zedoary dregs, comprising the following steps:
[0082] S1: drying zedoary dregs with hot air to a water content of 14% to obtain dried zedoary dregs. The hot air is obtained by heat exchange between coal flue gas and air, and the temperature of the coal flue gas is 940°C. The air temperature is 20°C, and the hot air temperature is 360°C;
[0083] S2: pulverize the dried zedoary dregs prepared in step S1, and pass through a 150-mesh sieve to obtain a pulverized dried zedoary dregs;
[0084] S3: Add a potassium hydroxide solution with a concentration of 15% to the dried zedoary dregs pulverized material obtained in step S2, and stir for 7 minutes at a rotating speed of 120 r / min, so that the zedoary dregs are completely immersed in the potassium hydroxide solution, And soaking at a temperature of 45°C for 18 hours to obtain pretreated curcuma dregs;
[0085] S4: Mix the zedoary dregs and sludge after the pretreatm...
Embodiment 2
[0110] A method for preparing methane and barbecue charcoal from zedoary dregs, comprising the following steps:
[0111] S1: Dried zedoary dregs with hot air to a moisture content of 13% to obtain dried zedoary dregs. The hot air was obtained by heat exchange between coal flue gas and air, and the temperature of the coal flue gas was 920°C. The air temperature is 4°C, and the hot air temperature is 250°C;
[0112] S2: pulverize the dried zedoary dregs prepared in step S1, and pass through a 100-mesh sieve to obtain a pulverized dried zedoary dregs;
[0113] S3: Add a potassium hydroxide solution with a concentration of 8% to the dried zedoary dregs pulverized material obtained in step S2, and stir for 8 minutes at a rotating speed of 80 r / min, so that the zedoary dregs are completely immersed in the potassium hydroxide solution, and soaked at a temperature of 42°C for 16 hours to obtain pretreated zedoary dregs;
[0114] S4: the zedoary dregs and the sludge after the pretrea...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com