[0025] A stone-plastic wallboard comprising the following raw materials: 50 grams of calcite powder, 40 grams of PVC resin, 20 grams of neoprene rubber, 33 grams of nitrile rubber, 3 grams of conductive fiber, 30 grams of marble powder, and 4 grams of processing aids , 4 grams of modifier, 1 gram of stabilizer, 2 grams of foaming agent, 1 gram of lubricant, 90 grams of hemihydrate gypsum, 1 gram of bamboo charcoal fiber, 2 grams of methyl cellulose, 3 grams of ethyl cellulose, imitation stone 20 grams of paint and 3 grams of polyvinyl alcohol.
[0026] The surface of the above-mentioned stone-plastic wallboard is coated with an anti-corrosion coating, and the raw materials of the anti-corrosion coating include by weight: 20 grams of acrylic resin, 30 grams of composite polybenzoxazine material, 10 grams of aldehyde and ketone resin KR-80F, lignin fiber 1 gram, 5 grams of conductive fiber, 1 gram of aluminum-zirconium coupling agent TL-4, 1 gram of curing agent, 1 gram of defoa...
Embodiment 2
[0038] A stone-plastic wallboard comprising the following raw materials: 80 grams of calcite powder, 60 grams of PVC resin, 30 grams of neoprene rubber, 43 grams of nitrile rubber, 5 grams of conductive fiber, 50 grams of marble powder, and 8 grams of processing aids , 8 grams of modifier, 3 grams of stabilizer, 5 grams of foaming agent, 5 grams of lubricant, 100 grams of hemihydrate gypsum, 3 grams of bamboo charcoal fiber, 5 grams of methyl cellulose, 7 grams of ethyl cellulose, imitation stone Paint 30 grams and polyvinyl alcohol 6 grams.
[0039] The surface of the above-mentioned stone-plastic wallboard is coated with anti-corrosion paint, and the raw materials of the anti-corrosion paint include by weight: 50 grams of acrylic resin, 50 grams of composite polybenzoxazine material, 20 grams of aldehyde and ketone resin KR-80F, paraffin wax 1 gram, 2 grams of zirconium chloride, 6 grams of lignin fiber, 8 grams of conductive fiber, 2 grams of aluminum-zirconium coupling age...
Embodiment 3
[0051] A stone-plastic wallboard, comprising the following raw materials: 65 grams of calcite powder, 50 grams of PVC resin, 25 grams of neoprene rubber, 38 grams of nitrile rubber, 4 grams of conductive fiber, 40 grams of marble powder, 6 grams of processing aids, modified 6 grams of neutralizing agent, 2 grams of stabilizer, 4 grams of foaming agent, 3 grams of lubricant, 95 grams of hemihydrate gypsum, 2 grams of bamboo charcoal fiber, 3 grams of methyl cellulose, 5 grams of ethyl cellulose, 35 grams of imitation stone paint gram and polyvinyl alcohol 4 grams.
[0052] The surface of the above-mentioned stone-plastic wallboard is coated with an anti-corrosion paint, and the anti-corrosion paint includes the following raw materials: 35 grams of acrylic resin, 40 grams of composite polybenzoxazine material, 15 grams of aldehyde and ketone resin KR-80F, 1 gram of paraffin, chlorinated 2 grams of zirconium, 4 grams of lignin fiber, 8 grams of conductive fiber, TL-41 grams of al...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com