Low-sulfur biomass rod fuel and preparation method thereof
A technology of biomass and rods, applied in the direction of biofuels, solid fuels, waste fuels, etc., can solve problems such as inability to meet environmental protection, environmental pollution, and low energy conversion efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] A low-sulfur biomass stick fuel proposed by the present invention, its raw materials include by weight: 50 parts of rice straw, 20 parts of wheat straw, 6 parts of giant fungus grass, 4.5 parts of elephant grass, 6.5 parts of reed bamboo, and 4 parts of corn cob , 5 parts of coal, 4.5 parts of lanthanum oxide, 3.5 parts of copper nitrate, 2.5 parts of cobalt nitrate, 6 parts of fluororesin, 3.5 parts of polymethacrylate, 4.5 parts of terexylylene resin, 3.5 parts of silicone resin, nitro 5 parts of cellulose, 6 parts of silane coupling agent KH-570, 6 parts of modified water-resistant environmental protection adhesive, 10 parts of adhesive reinforcing material, 10 parts of modified reinforcing filler, 6 parts of methyl ethyl ketone peroxide, 4 parts of isocyanate .
[0021] The modified water-resistant and environmentally friendly adhesive is prepared according to the following process: 10 parts by weight of polyether diol, 3.5 parts of toluene diisocyanate and 4.5 part...
Embodiment 2
[0028] A low-sulfur biomass rod fuel proposed by the present invention, its raw materials include by weight: 40 parts of rice straw, 25 parts of wheat straw, 4 parts of giant fungus grass, 6 parts of elephant grass, 4 parts of reed bamboo, and 6 parts of corn cob 2 parts of coal, 6 parts of lanthanum oxide, 2 parts of copper nitrate, 4 parts of cobalt nitrate, 3 parts of fluororesin, 5 parts of polymethacrylate, 3 parts of terexylylene resin, 5 parts of silicone resin, nitro 4 parts of cellulose, 8 parts of silane coupling agent KH-570, 4 parts of modified water-resistant environmental protection adhesive, 15 parts of adhesive reinforcing material, 5 parts of modified reinforcing filler, 8 parts of methyl ethyl ketone peroxide, 2 parts of isocyanate .
[0029] The modified water-resistant and environmentally friendly adhesive is prepared according to the following process: 5 parts of polyether diol, 5 parts of toluene diisocyanate and 3 parts of dibutyltin dilaurate are evenly...
Embodiment 3
[0036] A low-sulfur biomass rod fuel proposed by the present invention, its raw materials include by weight: 60 parts of rice straw, 15 parts of wheat straw, 8 parts of giant fungus grass, 3 parts of elephant grass, 9 parts of reed bamboo, and 2 parts of corncob 8 parts of coal, 3 parts of lanthanum oxide, 5 parts of copper nitrate, 1 part of cobalt nitrate, 9 parts of fluororesin, 2 parts of polymethacrylate, 6 parts of terexylylene resin, 2 parts of silicone resin, nitro 6 parts of cellulose, 4 parts of silane coupling agent KH-570, 8 parts of modified water-resistant environmental protection adhesive, 5 parts of adhesive reinforcing material, 15 parts of modified reinforcing filler, 4 parts of methyl ethyl ketone peroxide, 6 parts of isocyanate .
[0037] The modified water-resistant and environmentally friendly adhesive is prepared according to the following process: 15 parts of polyether diol, 2 parts of toluene diisocyanate and 6 parts of dibutyltin dilaurate are mixed u...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com