Matrix adopting nano-packaging technology and preparation method of matrix
A matrix and encapsulation technology, which is applied to the matrix of nano-encapsulation technology and its preparation field, can solve the problems of complicated preparation process, limited dosage form, high cost, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0040]Such asfigure 1 As shown, the present embodiment discloses a flow chart of a matrix preparation method of nano-wrap technology, which is as follows:
[0041]Add ion water soluble serum albumin to form 0.2% of the functional ingredient solution;
[0042]Add ion water to dissolve tanning acid to form 0.2% phytophenol solution;
[0043]Add ion water to dissolve zinc lactic acid, gluconate and manganese sulfate, and form 1.5% metal ion solution;
[0044]Add ion water (or acid-promoting) to dissolve chitosan and its derivatives, form 0.02% wall material solution;
[0045]Add ion water to dissolve the xanthan gum, Carropom, form 0.5% stable ingredient solution;
[0046]Add ion water to dissolve arginine, lysine, histidine, and form a 1% buffer moiety;
[0047]1 part of the metal ion solution, 10 parts of the plant polyphenol solution, 1 part of the stabilized component solution, 1 part of the wall material, mixed, stirred, and formed, forming a solution A.
[0048]1 part of the functional component solutio...
Embodiment 2
[0052]Such asfigure 1 As shown, the present embodiment discloses a flow chart of a matrix preparation method of nano-wrap technology, which is as follows:
[0053]Add ion water to dissolve aloe vera extracts to form a solution of 0.5% efficacy ingredient;
[0054]Add ion water to dissolve EGCG (the table did not eat the sercein without meal acid ester), forming 0.5% plant polyphenol solution;
[0055]Add ion water to dissolve the ferrous iron, citrate, copper, gluconate, and form a 2% metal ionic solution;
[0056]Add ion water to dissolve gelatin, pectin, deacemic, formation of 0.3% wall portion;
[0057]Add ion water to dissolve starch, dextran, form 0.01% stable partial solution;
[0058]Add ion water to dissolve potassium lactate, nicotinamide, and form a 3% buffer portion;
[0059]1 part of the metal ion solution, 10 parts of the plant polyphenol solution, 1 part of the stabilized component solution, 1 part of the wall material, mixed, stirred, and formed, forming a solution A.
[0060]1 part of the f...