Embodiment 1
[0030] 1. Potassium alginate 12 grams
[0031] 2. Glucomannan 2 grams
[0032] 3. Polylysine 12g
[0033] 4. β-glucan 0.2g
[0034] 5. Glycerin 10g
[0035] 6. Sodium acetate 3g
[0036] Component 1: Dissolve 7.5 grams of lithium magnesium silicate in 500 ml of physiological saline adjusted to pH 8.0 with 1 mol of sodium hydroxide and mix well, then add the above ingredients and stir until completely dissolved, pack in 5 ml bottles, and sterilize by high-temperature steam.
[0037] Component 2: The solidification solution is prepared into a 1.1% aqueous solution with calcium chloride, packed in 5ml bottles, and sterilized by high-temperature steam.
Embodiment 2
[0039] 1. Amidated low methoxyl pectin 6g
[0040] 2. Glucomannan 2g
[0041] 3 Potassium alginate 8g
[0042] 4. Chitosan 12g
[0043] 5. Oat glucan 0.2g
[0044] 6. Glycerin 10g
[0045] 7. Sodium gluconate 1g
[0046] Component 1: Dissolve 7.5 grams of lithium magnesium silicate in 500 ml of physiological saline adjusted to pH 8.0 with sodium bicarbonate and mix evenly, then add the above ingredients and stir until completely dissolved, pack in 5 ml bottles, and sterilize by high-temperature steam.
[0047] Component 2: The solidification solution is prepared into a 1.1% aqueous solution with calcium chloride, packed in 5ml bottles, and sterilized by high-temperature steam.
Embodiment 3
[0049] 1. Sodium alginate 12g
[0050] 2. Glucomannan 2.5g
[0051] 3. Polylysine 4g
[0052] 4. Oat glucan 0.2g
[0053] 5. Polyvinyl alcohol 2.5g
[0054] 6. Sodium citrate 5g
[0055] Component 1: Dissolve 7.5 grams of lithium magnesium silicate in 500 ml of physiological saline adjusted to pH 8.0 with 1 mol of sodium hydroxide and mix well, then add the above ingredients and stir until completely dissolved, pack in 5 ml bottles, and sterilize by high-temperature steam.
[0056] Component 2: The solidification solution is prepared into a 2% aqueous solution with calcium gluconate, packed in 5ml bottles, and sterilized by high-temperature steam.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com