A chlorine dioxide and disinfectant technology, applied in the direction of disinfectant, biocide, animal repellent, etc., can solve the problems of poor biodegradability, short storage time, affecting product production cost and performance, and achieve high conversion rate , Less effect of chlorite
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] Weigh 21 kg of anhydrous zinc sulfate, dry and fully pulverize into fine powder, then divide into three equal parts for later use. Mix 7 kg of anhydrous zinc sulfate powder and 10 kg of sodium chlorite in an airtight container, and dry in a dryer at 115°C for 20 minutes to make the first component; 7 kg of zinc sulfate water powder and 14 kg of sodium persulfate were mixed evenly in a closed container, and dried in a dryer at 120 ° C for 15 minutes to make the second component; another part of zinc sulfate anhydrous powder 7 kg 1 kg and 6.5 kg of maleic acid are mixed evenly in a closed container, and dried in a dryer at 110°C for 20 minutes to make the third component; add the third component to the second component, and mix well Then add it to the first component, and pack it in separate bags with moisture-proof materials after mixing.
Embodiment 2
[0019] Weigh 20 kg of anhydrous zinc sulfate, dry and fully pulverize into fine powder, then divide into two equal parts for later use. Mix 10 kg of anhydrous zinc sulfate powder and 10 kg of sodium chlorite in a closed container, and dry in a dryer at 115°C for 20 minutes to make the first component; Mix 10 kg of anhydrous zinc sulfate powder with 13.5 kg of sodium persulfate and 7.5 kg of malic acid in a closed container, and dry in a dryer at 110°C for 20 minutes to make the second component; Add it to the first component, mix evenly, then dry it in a dryer at 120°C for 10 minutes, and pack it in separate bags with moisture-proof materials.
Embodiment 3
[0021] Weigh 18 kg of anhydrous sodium sulfate, dry and fully pulverize into fine powder, then divide into three equal parts for later use. Mix 6 kg of anhydrous sodium sulfate powder and 10 kg of sodium chlorite in a closed container, and dry in a dryer at 115°C for 20 minutes to make the first component; Mix 6 kg of sodium sulfate water powder and 15 kg of sodium persulfate in a closed container, and dry in a dryer at 120 ° C for 15 minutes to make the second component; another part of sodium sulfate anhydrous powder 6 1 kg and 6.5 kg of maleic acid are mixed evenly in a closed container, and dried in a dryer at 110°C for 20 minutes to make the third component; add the third component to the second component, and mix well Then add it to the first component, and pack it in separate bags with moisture-proof materials after mixing.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com