Anticorrosive coating material and preparation method therefor
A technology of anti-corrosion coatings and raw materials, applied in the direction of anti-corrosion coatings, polyester coatings, epoxy resin coatings, etc., can solve the problems of easy peeling off of protective coatings, corrosion, and affecting the durability and appearance of water tanks, so as to improve hardness and feel, durability Strong corrosion resistance and excellent performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] A kind of anticorrosion paint raw material comprises 45 parts of epoxy resins, 15 parts of unsaturated polyester resins, 8 parts of propylene glycidyl ethers, 2 parts of aluminum tripolyphosphate, 18 parts of micaceous iron oxides, 9 parts of iron oxide reds in parts by weight , 16 parts of talc powder, 12 parts of glass powder, 1.2 parts of nano-alumina, 2.5 parts of nano-titanium dioxide, 2.5 parts of bentonite, 1.5 parts of dipropylene glycol methyl ether, 1.5 parts of alcohol ester-12, 2 parts of thixotropic polyacrylate, triphosphate 3 parts of butyl ester, 1.5 parts of acrylate copolymer.
[0021] The method for preparing above anti-corrosion coating is characterized in that: comprises the following steps:
[0022] (1) Mix epoxy resin, unsaturated polyester resin, and acryl glycidyl ether in a paint mixer to obtain a mixed solution;
[0023] (2) Add aluminum tripolyphosphate, mica iron oxide, iron oxide red, talc powder, glass powder, nano-alumina, nano-titanium ...
Embodiment 2
[0026] A kind of anti-corrosion paint raw material comprises 48 parts of epoxy resin, 18 parts of unsaturated polyester resin, 9 parts of butyl glycidyl ether, 3 parts of aluminum tripolyphosphate, 22 parts of micaceous iron oxide, 14 parts of iron oxide red in parts by weight , 19 parts of talcum powder, 14 parts of glass powder, 1.8 parts of nano-alumina, 3.5 parts of nano-titanium dioxide, 4 parts of fumed silica, 2 parts of dipropylene glycol methyl ether, 3 parts of alcohol ester-12, 4 parts of thixotropic polyacrylate , 5 parts of polysiloxane-polyether copolymer, 2 parts of fluorine-modified polyacrylate copolymer, and 1.5 parts of polyester-modified polysiloxane.
[0027] The method for preparing above-mentioned anticorrosion coating comprises the following steps:
[0028] (1) Mix epoxy resin, unsaturated polyester resin, and reactive diluent in a paint mixer to obtain a mixed solution;
[0029] (2) Add aluminum tripolyphosphate, micaceous iron oxide, iron oxide red, ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com