Biomass synthetic resin and method for producing coconut palm mattress by use of biomass synthetic resin as adhesive

A synthetic resin and biomass technology, which is applied in the preparation of adhesives, starch-derived adhesives, animal glue or gelatin, etc., can solve the problem of excessive free formaldehyde content in adhesives, achieve good bonding performance, improve bonding performance, reduce The effect of viscosity

Inactive Publication Date: 2017-05-17
郑州佰沃科技发展有限公司
View PDF4 Cites 13 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0005] The main disadvantage of urea-formaldehyde resin is reflected in environmental protection
In order to ensure the bonding strength, urea-formaldehyde resin with a relatively large molar ratio is often used in actual production, resulting in excessive free formaldehyde content in the adhesive.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0036] The biomass synthetic resin of the present invention, the biomass synthetic resin is prepared by the following method:

[0037] a, expressed in parts by weight, the biomass synthetic resin is composed of 30 parts of defatted soybean protein powder, 20 parts of pea protein powder, 35 parts of oxidized corn starch and 8 parts of cellulose sulfate;

[0038] b. Weighing 10 parts by weight of urea and 0.1 part by weight of N-butylthiophosphoric triamide were dissolved in 100 parts by weight of water to prepare a chain extender solution;

[0039] c. Stir and add various raw materials prepared according to the ratio of biomass synthetic resin described in step a to the chain extender solution prepared in step b, and then stir and react at room temperature for 40 minutes;

[0040] d. Heat the normal temperature reaction product obtained in step c to 60° C., and react at this temperature for 50 minutes; after the reaction is completed, the obtained reactant drops to 35° C.;

[...

Embodiment 2

[0043] The biomass synthetic resin of the present invention, the biomass synthetic resin is prepared by the following method:

[0044]a, expressed in parts by weight, the biomass synthetic resin consists of 30 parts of defatted peanut flour, 30 parts of rapeseed cake powder, 20 parts of esterified potato starch, 20 parts of esterified corn starch and 10 parts of cellulose xanthic acid Ester composition;

[0045] b. Take 15 parts by weight of thiourea and dissolve it in 100 parts by weight of water to prepare a chain extender solution;

[0046] c. Stir and add various raw materials prepared according to the ratio of biomass synthetic resin described in step a to the chain extender solution prepared in step b, and then stir and react at room temperature for 35 minutes;

[0047] d. Heating the normal temperature reaction product obtained in step c to 80° C., and reacting at this temperature for 30 minutes; after the reaction is completed, the obtained reactant is lowered to 30° ...

Embodiment 3

[0050] The biomass synthetic resin of the present invention, the biomass synthetic resin is prepared by the following method:

[0051] a, expressed in parts by weight, the biomass synthetic resin is composed of 25 parts of defatted cottonseed powder, 10 parts of wheat gluten powder, 5 parts of casein powder, 35 parts of esterified tapioca starch and 5 parts of hydroxypropyl methylcellulose ;

[0052] b. Take 6 parts by weight of sodium lauryl sulfate and dissolve it in 100 parts by weight of water to prepare a chain extender solution;

[0053] c. Stir and add various raw materials prepared according to the ratio of biomass synthetic resin described in step a to the chain extender solution prepared in step b, and then stir and react at room temperature for 50 minutes;

[0054] d. Heat the normal temperature reaction product obtained in step c to 85° C., and react at this temperature for 35 minutes; after the reaction is completed, the obtained reactant drops to 40° C.;

[005...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses biomass synthetic resin and method for producing a coconut palm mattress by use of the biomass synthetic resin as an adhesive. The biomass synthetic resin is obtained through the following steps: mainly taking biomass synthetic resin albumen powder, modified starch and modified cellulose as main raw materials, preparing a chain extender as a solution, adding the main raw materials to react at a normal temperature, and then heating to perform the reaction, cooling after the reaction, orderly adding a cross-linking agent, a tackifier and an inorganic filler to stir and react to obtain a product biomass synthetic resin. The method for producing the coconut palm mattress by use of the biomass synthetic resin as an adhesive is as follows: firstly treating bundled coconut palm raw material into the coconut palm fiber, carding through a coconut shred carding machine, and then weaving as a curtain through a lapping machine; sizing and folding the curtain by use of a spraying sizing system to obtain a coconut palm blank; and then performing the prepressing molding, hot-pressing molding and after-treatment in order to obtain the product coconut palm mattress. The biomass synthetic resin adhesive disclosed by the invention is virtually formaldehyde and organic volatile matter-free, and the harm to the human body health in the use process is avoided.

Description

technical field [0001] The invention belongs to the technical field of household bedding processing, and in particular relates to a biomass synthetic resin and a method for producing coconut palm mattresses using the biomass synthetic resin as an adhesive. Background technique [0002] At present, the main raw materials used in the processing and production of palm mattresses are mountain palm and coconut palm. Mountain palm mainly grows in the southwestern region of my country. After many years of growth, the palm fiber is suitable for making mattresses. Each palm can only harvest a few pieces of brown chips and brown boards every year. After several complex pretreatment processes, the fiber material can be As a raw material for brown mattresses. Coconut palm is made of coconut shell, and the fiber silk is extracted as the raw material of palm mattress. Mountain palm has the advantages of long fiber, resistance to insects, high strength, and good toughness. It can be proce...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): C09J4/06C09J4/02C09J11/08C09J11/04C09J189/00C09J103/06C09J101/22C09J101/28
CPCC08L2205/025C08L2205/035C09J4/06C09J11/04C09J11/08C09J103/06C09J189/00C08L89/00C08L3/06C08L1/22C08L77/00C08L63/00C08K3/346C08L1/284C08L33/04C08K3/38
Inventor 陈锡建杨立新曹新华成宇陈奕州陶杰吴军强宁有才张晓亚
Owner 郑州佰沃科技发展有限公司
Features
  • Generate Ideas
  • Intellectual Property
  • Life Sciences