Anti-oxidative refractory brick and preparation method thereof

A refractory brick and anti-oxidation technology, applied in the field of refractory materials, can solve the problems of low refractoriness, low strength and high cost, and achieve the effects of high wear resistance, low expansion coefficient and improved thermal stability

Inactive Publication Date: 2017-05-24
MAANSHAN BAOLONG NEW BUILDING MATERIALS
View PDF4 Cites 5 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

The invention provides a foamed thermal insulation refractory brick produced using coal gangue as the main raw material and its preparation method, although it solves the problems of low refractoriness, poor molding, low strength and high cost of lightweight refractory thermal insulation bricks in the

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment Construction

[0016] An anti-oxidation refractory brick made of the following raw materials in parts by weight: 12-19 parts by weight of quartzite, 10-15 parts by weight of topaz, 11-17 parts of coal water slurry slag, 5-10 parts of silicon oxynitride, and 18-27 parts by weight of dolomite , zirconium diboride 7-13, forsterite 8-16, dolomite 9-18, marine dredging mud 22-29, anthracite 16-24, granite gravel 14-22, kaolin 15-20, porous powder quartz 10 -15, pyrophyllite 5-10, industrial alumina 13-19.

[0017] A method for preparing an anti-oxidation refractory brick, comprising the following steps:

[0018] (1) Mix quartzite, forsterite, and dolomite evenly, crush them, pass through a 80-120 mesh sieve, add sodium carbonate equivalent to 40-50% of the mixed powder mass and 35-45% sodium nitrate, 500-800r / min dry ball milling for 15-25min, then calcined at 860-920°C for 4-6h, and cooled to room temperature;

[0019] (2) Mix topaz, pyrophyllite, and industrial alumina evenly, crush them, pa...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses an anti-oxidative refractory brick and a preparation method thereof. The anti-oxidative refractory brick is prepared from raw materials in parts by weight as follows: 12-19 parts of quartzite, 10-15 parts of topaz, 11-17 parts of coal water slurry slag, 5-10 parts of silicon oxynitride, 18-27 parts of dolomite, 7-13 parts of zirconium diboride, 8-16 parts of forsterite, 9-18 parts of dolomite, 22-29 parts of marine dredged sludge, 16-24 parts of anthracite, 14-22 parts of granite stones, 15-20 parts of kaolin, 10-15 parts of porous powder quartz, 5-10 parts of pyrophyllite and 13-19 parts of industrial aluminum oxide. The effects of promoting sintering and improving the oxidation resistance and the corrosion resistance of the refractory brick are realized by introducing silicon oxynitride and zirconium diboride; the added raw materials such as porous powder quartz, coal water slurry slag and the like can improve the heat stability, the corrosion resistance and the wear resistance of the refractory brick. The refractory brick has excellent properties of excellent oxidation resistance, thermal shock resistance, corrosion resistance, wear resistance, high high-temperature strength, low expansion coefficients and the like.

Description

technical field [0001] The invention relates to an anti-oxidation refractory brick and a preparation method thereof, belonging to the field of refractory materials. Background technique [0002] Refractory brick is a kind of building material brick, and its property is "refractory" like its name. It is a refractory material fired from refractory clay or other refractory raw materials, which can withstand various physical and chemical changes and mechanical actions at high temperatures. Refractory bricks are not common in our lives, but they appear in some buildings that are closely related to our lives, such as housing construction, kiln construction, thermal equipment, etc. [0003] The invention patent with the patent number: 201510494613.X discloses a foamed thermal insulation refractory brick produced by using coal gangue and its preparation method. The raw material composition is 40-60 parts by weight of coal gangue, bauxite tailings 30-50 parts, 2-15 parts of fly ash...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): C04B35/66C04B33/13C04B33/135C04B33/132
CPCC04B33/13C04B33/131C04B33/1321C04B33/1324C04B33/135C04B35/66C04B2235/321C04B2235/3217C04B2235/3418C04B2235/3445C04B2235/3813C04B2235/3873C04B2235/422C04B2235/96C04B2235/9607C04B2235/9684Y02P40/60
Inventor 晋元龙陈德全
Owner MAANSHAN BAOLONG NEW BUILDING MATERIALS
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products