High-purity ferro-titanium pearlescent pigment with bright golden yellow effect and preparation method thereof
A technology of ferro-titanium and pearlescent pigments, which is applied in the field of pearlescent pigments, can solve problems such as large application limitations, high use risks, and large safety hazards in production, and achieve the effects of simple production process, stable scale production, and strong operability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] A kind of preparation method of high-purity ferro-titanium alloy shining golden color effect pearlescent pigment, comprises the following steps: the first step, in 1 liter glass beaker, add 500 milliliters of water, throw 30-40 gram 10-60 micron synthetic mica substrate, Start stirring at 260-300 rpm, heat up to 70-75°C, add 8% hydrochloric acid aqueous solution to adjust pH to 1.5-1.8, after adjustment, stir for 10-30 minutes; the second step is to add 10% Aqueous solution of tin tetrachloride, add 16% aqueous sodium hydroxide solution dropwise, keep the pH constant, after feeding for 30 minutes, stir for 10-20 minutes; in the third step, increase the rotating speed to 300-360 rpm, and heat up to 78 -82°C, use 16% sodium hydroxide aqueous solution to raise the pH to 1.9-2.2, slowly add 2M titanium tetrachloride dropwise, control the dropping time for 5-7 hours, and add 16% sodium hydroxide aqueous solution dropwise to keep the pH value constant , add dropwise until the...
Embodiment 2
[0015]A kind of preparation method of high-purity ferro-titanium alloy shining golden color effect pearlescent pigment, comprises the following steps: the first step, in 1 liter glass beaker, add 500 milliliters of water, throw 30-40 gram 10-60 micron synthetic mica substrate, Start stirring at 260-300 rpm, heat up to 70-75°C, add 8% hydrochloric acid aqueous solution to adjust pH to 1.5-1.8, after adjustment, stir for 10-30 minutes; the second step is to add 10% 30 ml of zinc dichloride aqueous solution, and 16% sodium hydroxide aqueous solution was added dropwise to keep the pH constant. After 30 minutes of feeding, stir for 10-20 minutes; the third step, increase the rotating speed to 300-360 rpm, and heat up When the temperature is 78-82°C, use 16% sodium hydroxide aqueous solution to raise the pH to 1.9-2.2, slowly add 2M titanium tetrachloride dropwise, control the dropping time for 5-7 hours, and add 16% sodium hydroxide aqueous solution dropwise to maintain the pH When...
Embodiment 3
[0017] A kind of preparation method of high-purity ferro-titanium alloy shining golden color effect pearlescent pigment, comprises the following steps: the first step, in 1 liter glass beaker, add 500 milliliters of water, throw 30-40 gram 10-60 micron synthetic mica substrate, Start stirring at 260-300 rpm, heat up to 70-75°C, add 8% hydrochloric acid aqueous solution to adjust pH to 1.5-1.8, after adjustment, stir for 10-30 minutes; the second step is to add 10% Add 30 ml of stannous chloride aqueous solution, and add 16% aqueous sodium hydroxide solution dropwise to keep the pH constant. After 30 minutes of feeding, stir for 10-20 minutes; in the third step, increase the rotating speed to 300-360 rpm, and heat up When the temperature is 78-82°C, use 16% sodium hydroxide aqueous solution to raise the pH to 1.9-2.2, slowly add 2M titanium tetrachloride dropwise, control the dropping time for 5-7 hours, and add 16% sodium hydroxide aqueous solution dropwise to maintain the pH ...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com