A water-based coating, corrosion-resistant technology, applied in anti-corrosion coatings, anti-fouling/underwater coatings, fire-resistant coatings, etc., can solve problems such as poor bonding strength, and achieve the effects of protection strength, good thermal insulation performance, and enhanced adhesion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] A kind of corrosion-resistant water-resistant water-based coating that the present invention proposes, its raw material comprises by weight: 20 parts of epoxy resins, 80 parts of saturated linear polyester resins, 1 part of pine tar, 25 parts of polyethylene waxes, dodecylbenzenesulfonate 1.2 parts of sodium bicarbonate, 15 parts of ethylene glycol, 0.8 parts of calcium sorbate, 2 parts of rosin resin, 2 parts of thickener, 4 parts of crosslinking agent, 2 parts of pigment, 80 parts of filler, 40 parts of water.
Embodiment 2
[0016] A kind of corrosion-resistant water-resistant water-based coating that the present invention proposes, its raw material comprises by weight: 30 parts of epoxy resins, 60 parts of saturated linear polyester resins, 2 parts of pine tars, 15 parts of polyethylene waxes, dodecylbenzene sulfonate 2 parts of sodium bicarbonate, 10 parts of ethylene glycol, 1.4 parts of calcium sorbate, 1 part of rosin resin, 4 parts of thickener, 2 parts of cyclohexanone peroxide, 4 parts of pigment, 70 parts of filler, and 60 parts of water.
[0017] The filler includes, in parts by weight: 10 parts of nano silicon dioxide, 15 parts of nano montmorillonite, 4 parts of nano cellulose whisker, 7 parts of calcined clay, 8 parts of wood fiber composite and 6 parts of polyborate fiber.
[0018] The lignocellulosic composite is prepared by the following process: add water to the soybean powder, treat it with a rubber mill, add polyethylene wax, heat up and stir, add wood fiber, tungalic anhydride m...
Embodiment 3
[0020] A corrosion-resistant water-resistant water-based paint proposed by the present invention, its raw materials include by weight: 22 parts of epoxy resin, 75 parts of saturated linear polyester resin, 1.2 parts of pine tar, 22 parts of polyethylene wax, dodecylbenzenesulfonate 1.4 parts of sodium bicarbonate, 14 parts of ethylene glycol, 1 part of calcium sorbate, 1.8 parts of rosin resin, 2.5 parts of thickener, 3.5 parts of cyclohexanone peroxide, 2.5 parts of pigment, 78 parts of filler, and 45 parts of water.
[0021] The filler includes, in parts by weight: 16 parts of nano silicon dioxide, 8 parts of nano montmorillonite, 8 parts of nano cellulose whisker, 5 parts of calcined clay, 12 parts of wood fiber composite, and 2 parts of polyborate fiber.
[0022] The wood fiber composite is prepared by the following process: add water to 18 parts of soybean flour in parts by weight, treat with rubber mill, add 30 parts of polyethylene wax, heat up and stir, add 15 parts of ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com