An environmentally friendly paint and raw material technology, which is applied to biocide-containing paints, rosin coatings, polyamide coatings, etc., can solve the problems of high raw material costs and unsuitability for large-scale industrialized production, and achieve good spreadability, bright color, moderate drying time
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] An environmentally friendly paint material, comprising the following raw materials in parts by weight: 19 parts of polyamide resin, 27 parts of acrylic resin, 15 parts of calcium carbonate powder, 3 parts of rosin, 10 parts of zinc oxide, 10 parts of tartaric acid, 4 parts of plant essential oil, chlorinated 7 parts of paraffin, 11 parts of sodium carboxymethyl cellulose, 4 parts of dibutyltin dilaurate, 10 parts of oil resistance additives, 4 parts of glacial acetic acid, 14 parts of dilution solvent, 5 parts of stabilizer, 13 parts of color paste and deionized 9 parts of water.
[0030] A preparation method for an environmentally friendly paint material, comprising the following preparation steps:
[0031] a. Mix calcium carbonate powder, chlorinated paraffin and deionized water, stir and disperse at a speed of 400r / min for 20min, then add polyamide resin and acrylic resin, heat up to 87°C, keep warm for 1.1h, and cool to obtain the material one;
[0032] b. Import ...
Embodiment 2
[0041] An environmentally friendly paint material, comprising the following raw materials in parts by weight: 24 parts of polyamide resin, 25 parts of acrylic resin, 15 parts of calcium carbonate powder, 6 parts of rosin, 7 parts of zinc oxide, 9 parts of tartaric acid, 7 parts of plant essential oil, chlorinated 7 parts of paraffin wax, 8 parts of sodium carboxymethyl cellulose, 4 parts of dibutyltin dilaurate, 7 parts of oil resistance additives, 4 parts of glacial acetic acid, 12 parts of dilution solvent, 10 parts of stabilizer, 8 parts of color paste and deionized 14 parts of water.
[0042] A preparation method for an environmentally friendly paint material, comprising the following preparation steps:
[0043] a. Mix calcium carbonate powder, chlorinated paraffin and deionized water, stir and disperse at a speed of 500r / min for 25min, then add polyamide resin and acrylic resin, heat up to 87°C, keep warm for 0.8h, and cool to obtain the material one;
[0044] b. Import...
Embodiment 3
[0053] An environmentally friendly paint material, comprising the following raw materials in parts by weight: 22 parts of polyamide resin, 24 parts of acrylic resin, 14 parts of calcium carbonate powder, 5 parts of rosin, 8 parts of zinc oxide, 7 parts of tartaric acid, 7 parts of plant essential oil, chlorinated 10 parts of paraffin wax, 10 parts of sodium carboxymethyl cellulose, 6 parts of dibutyltin dilaurate, 9 parts of oil resistance additives, 5 parts of glacial acetic acid, 10 parts of dilution solvent, 8 parts of stabilizer, 9 parts of color paste and deionized 12 parts of water.
[0054] A preparation method for an environmentally friendly paint material, comprising the following preparation steps:
[0055] a. Mix calcium carbonate powder, chlorinated paraffin and deionized water, stir and disperse at a speed of 500r / min for 20min, then add polyamide resin and acrylic resin, heat up to 87°C, keep warm for 0.8h, and cool to obtain the material one;
[0056] b. Impor...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com