A kind of environment-friendly high-performance coating inhibitor and its preparation method and application
A coating inhibitor, high-performance technology, applied in chemical instruments and methods, drilling compositions, etc., can solve the problems of the coating inhibition effect needs to be further strengthened, the complete dissolution time is long, and the mud filtration volume increases. , to achieve the effect of outstanding environmental protection performance, easy filtration and purification, and low production energy consumption
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0038] (1) First add 800kg of distilled water, 400kg of isopropanol and 700kg of ethylene glycol into the reaction kettle, stir to mix evenly, and use it as a polymerization solvent for later use.
[0039](2) Add 475 kg of the first monomer N, N-dimethylacrylamide and 325 kg of 2-acrylamido-2-methylpropanesulfonic acid, and the second monomer N-(3-aminopropyl) methyl Acrylic acid ammonium salt 320kg, the third monomer 1-vinyl-2-pyrrolidone 60kg, initiator pentaerythritol 2.0kg, and dispersion stabilizer polyoxyethylene diamine 16kg, add in (1), stir to make it dissolve completely, then 2.0 kg of initiator ammonium persulfate was dissolved in 100 kg of distilled water and placed in a constant pressure dropping funnel; ammonia water was added to adjust the pH of the solution to 8.5. Introduce nitrogen protection into the reaction kettle and keep it for 30 minutes; then start to add ammonium persulfate aqueous solution dropwise and complete the dropwise addition within 15-25 minu...
Embodiment 2
[0041] (1) Add 700kg of distilled water, 600kg of isopropanol and 600kg of ethylene glycol into the reaction kettle, stir to mix evenly, and set aside as a polymerization solvent.
[0042] (2) the first monomer N, N'-(1,2-dihydroxyethylene) diacrylamide 410kg and 2-acrylamido-2-methylpropanesulfonic acid 300kg, the second monomer N-( 3-aminopropyl) methacrylic acid sodium salt 400kg, the third monomer 1-vinyl-2-pyrrolidone 14kg, initiator sodium persulfate 1.0kg, and dispersion stabilizer dimethyl diallyl ammonium chloride / Add 54 kg of acrylamide copolymer into (1), stir to make it dissolve completely, then dissolve 1.0 kg of the initiator sodium bisulfite in 100 kg of distilled water, and place it in a constant-pressure dropping funnel; add ammonia water to adjust the pH of the solution to 8.5. Introduce nitrogen protection into the reaction kettle and keep it for 30 minutes; then start to add aqueous sodium bisulfite solution dropwise and complete the dropwise addition wit...
Embodiment 3
[0044] (1) First add 840kg of distilled water, 560kg of ethylene glycol and 500kg of isopropanol into the reaction kettle, stir to mix evenly, and use it as a polymerization solvent for later use.
[0045] (2) N, N'-(1,2-dihydroxyethylene) diacrylamide 455kg and 2-acrylamido-2-methylpropanesulfonic acid 305kg, the second monomer N-(3-aminopropyl base) methacrylate ammonium salt 346kg, the third monomer 1-vinyl-2-pyrrolidone 50.4kg, initiator sodium persulfate 1.8kg, and dispersion stabilizer maleimide-based polyethylene glycol monomethyl ether 40kg , add in (1), stir to make it dissolve completely, then dissolve 1.8kg of initiator sodium bisulfite in 100kg of distilled water, place in a constant pressure dropping funnel; add ammonia water to adjust the pH value of the solution to 8.5. Introduce nitrogen protection into the reaction kettle and keep it for 30 minutes; then start to add aqueous sodium bisulfite solution dropwise, and complete the dropwise addition within 15-25 mi...