A kind of intermediate paint with excellent sealing performance and preparation method thereof
An intermediate paint, an excellent technology, applied in coatings, polyurea/polyurethane coatings, anti-corrosion coatings, etc., can solve the problems of epoxy resins such as poor aging resistance, general sealing performance, and easy chalking, and achieve low cost and high anti-corrosion performance Excellent, good sealing effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0024] An intermediate paint with excellent sealing performance, prepared by weighing the following raw materials:
[0025] 100 grams of phosphorus polyol (Exolit OP560), 17 grams of polyester resin (polycarbonate diol), 10 grams of dispersant BYK-307, 5 grams of zinc stearate (the role of zinc stearate is to make the paint easy to sand , convenient to continue painting on its surface), 1 gram of pigment, 10 gram of filler (titanium dioxide), 0.1 gram of polyether defoamer, 2 gram of anti-settling agent (polyethylene wax), 0.1 gram of leveling agent BYK-S706 , 171 grams of diluent (ethyl acetate) and 133 grams of curing agent TDI.
[0026] Prepare an intermediate paint with excellent sealing performance according to the following steps:
[0027] Step 1, add 17 grams of polyester resin to the paint mixing tank, then add 35 grams of ethyl acetate to it, and start stirring at a stirring speed of 400-600 rpm until a vortex appears in the center of the liquid surface;
[0028] St...
Embodiment 2
[0032] An intermediate paint with excellent sealing performance, prepared by weighing the following raw materials:
[0033] 450 grams of phosphorus polyol (Exolit OP560), 175 grams of polyester resin (polycaprolactone diol), 45 grams of dispersant BYK-330, 23 grams of zinc stearate, 4 grams of pigment, 50 grams of filler (calcium carbonate and mica powder mixture), 0.5 g polyether defoamer, 9 g anti-settling agent (bentonite), 0.5 g leveling agent BYK-S706, 830 g diluent (butyl acetate and xylene mixture) and 660 g curing agent TDI-TMP adduct.
[0034] The preparation method of the intermediate paint of this embodiment is the same as the preparation method of the intermediate paint of embodiment 1.
Embodiment 3
[0036] An intermediate paint with excellent sealing performance, prepared by weighing the following raw materials:
[0037] 900 grams of phosphorus polyol (ExolitOP560), 750 grams of polyester resin (adipic acid polyester polyol), 90 grams of dispersant BYK-330, 50 grams of zinc stearate, 10 grams of pigment, 100 grams of filler (talc Powder), 1 gram of polyether modified silicon defoamer, 45 grams of anti-settling agent (polyamide wax), 1 gram of leveling agent BYK-S706, 1870 grams of thinner (methyl ethyl ketone) and 1520 grams of curing agent TDI-TMP plus into things.
[0038] The preparation method of the intermediate paint of this embodiment is the same as the preparation method of the intermediate paint of embodiment 1.
PUM