Composite sludge deep dehydration agent and preparation method and use method thereof
A deep dehydration and sludge technology, which is applied in the sludge treatment of industrial sludge and municipal sludge, can solve the problems of high organic matter content, high conditioning time, unfavorable incineration, etc., and achieve the improvement of dehydration performance and compressive strength, saving Treatment cost, effect of reducing sludge volume
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
no. 1 example
[0019] In the first embodiment, the composition of the modifying agent is 80 parts of magnesium sulfate, 40 parts of aluminum sulfate, 10 parts of iron sulfate, 5 parts of ammonium sulfate, and 25 parts of magnesium oxide. It is prepared by the following steps: add 20% magnesium sulfate solution, 30% iron sulfate solution, and 30% aluminum sulfate solution to the reaction kettle, carry out high-temperature reaction after mixing, the reaction temperature is 50°C, and the reaction time is 6h; after the reaction is completed, the The mixed liquid is cooled, ammonium sulfate is added, mixed and stirred for 1 hour to obtain the first polymerization liquid; 50% magnesium oxide is made into a slurry, added to the first polymerization liquid, mixed and reacted for 6 hours to obtain the second polymerization liquid; The modifier is obtained by drying the second polymerization solution. The modifier and water are mixed at a mass ratio of 1:1 to 1:5 to prepare a modifier solution.
[00...
no. 2 example
[0021] In the second embodiment, the composition of the modifying agent is 5 parts of sodium aluminate, 30 parts of sodium gluconate, 70 parts of aluminum sulfate, and 10 parts of ferric chloride. Prepared through the following steps: add 50% sodium aluminate solution and 50% sodium gluconate solution to the reaction kettle and mix and stir for 4 hours to obtain an alkaline reaction solution; mix and stir 30% aluminum sulfate solution and 40% ferric chloride solution for 1 hour , to obtain an acidic reaction solution; under high-speed stirring conditions, slowly add the alkaline reaction solution into the acidic reaction solution to obtain a polymerization solution, and the stirring speed is 20r / min; dry the polymerization solution to obtain the modified agent. The modifier and water are mixed at a mass ratio of 1:1 to 1:5 to prepare a modifier solution.
[0022] The organic matter content of the sludge to be treated is 35%, and the moisture content of the sludge is 85% after...
no. 3 example
[0023] The third embodiment, the composition of modifying agent is the magnesium chloride of 60 parts, the magnesium sulfate of 40 parts, the aluminum sulfate of 30 parts, the ammonium chloride / sodium gluconate of 20 parts, the magnesium oxide of 10 parts, the coke of 5 parts sodium sulfate. It is prepared by the following steps: add 20% magnesium sulfate solution, 30% magnesium chloride solution, and 30% aluminum sulfate solution to the reaction kettle and mix them to carry out high-temperature reaction. The reaction temperature is 80°C and the reaction time is 6h; cooling, adding ammonium chloride and sodium gluconate, mixing and stirring for 1 hour to obtain the first polymerization liquid; making 50% magnesium oxide into a slurry, adding the first polymerization liquid, and mixing and reacting for 6 hours to obtain the second polymerization liquid; adding sodium pyrosulfate to the second polymerization liquid, adjusting the pH value of the sludge to 1-5 to obtain a primary...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com