Natural gas rare earth nano energy-saving additive
A technology of natural gas and additives, applied in the direction of gas fuel, petroleum industry, fuel, etc., can solve the problem of excessive toxic gas, and achieve the effect of promoting full combustion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] A natural gas rare earth nano energy-saving additive, the specific preparation method is as follows:
[0020] (1) Weigh the following parts by weight of the organic reagent solution, and mix it uniformly by ultrasonic
[0021] 25 parts of n-butanol, 25 parts of isopropanol, 18 parts of acetone, 8 parts of isobutanol, 5 parts of n-octanol, 8 parts of trimethylmethanol, 8 parts of methyl isobutyl ketone, methyl tert-butyl ether 3 copies;
[0022] (2) Preparation of rare earth solution
[0023] Ferrocene, nickel acetate and cerium oxide are mixed according to a weight ratio of 97.8:2:0.2, dissolved in an ethanol solvent to prepare a rare earth solution with a mass concentration of 10%;
[0024] (3) Add 5wt% rare earth solution to the organic reagent solution, put it aside for 24 hours after ultrasonic mutual dissolution, and obtain the natural gas rare earth nanometer energy-saving additive.
[0025] Add the above-mentioned additives quantitatively into the natural gas,...
Embodiment 2
[0027] A natural gas rare earth nano energy-saving additive, the specific preparation method is as follows:
[0028] (1) Weigh the following parts by weight of the organic reagent solution, and mix it uniformly by ultrasonic
[0029] 20 parts of n-butanol, 28 parts of isopropanol, 15 parts of acetone, 10 parts of isobutanol, 4 parts of n-octanol, 7 parts of trimethylmethanol, 5 parts of methyl isobutyl ketone, methyl tert-butyl ether 5 copies;
[0030] (2) Preparation of rare earth solution
[0031] Ferrocene, nickel acetate, and cerium oxide are mixed according to a weight ratio of 97.8:2:0.2, dissolved in an ethanol solvent to prepare a rare earth solution with a mass concentration of 10%;
[0032] (3) Add 5wt% rare earth solution to the organic reagent solution, put it aside for 24 hours after ultrasonic mutual dissolution, and obtain the natural gas rare earth nanometer energy-saving additive.
[0033] Add the above-mentioned additives to natural gas and do combustion e...
Embodiment 3
[0035] A natural gas rare earth nano energy-saving additive, the specific preparation method is as follows:
[0036] (1) Weigh the following parts by weight of the organic reagent solution, and mix it uniformly by ultrasonic
[0037] 30 parts of n-butanol, 30 parts of isopropanol, 20 parts of acetone, 5 parts of isobutanol, 4 parts of n-octanol, 8 parts of trimethylmethanol, 5 parts of methyl isobutyl ketone, methyl tert-butyl ether 5 copies;
[0038] (2) Preparation of rare earth solution
[0039] Ferrocene, nickel acetate and cerium oxide are mixed according to a weight ratio of 97.8:2:0.2, dissolved in an ethanol solvent to prepare a rare earth solution with a mass concentration of 10%;
[0040] (3) Add 5wt% rare earth solution to the organic reagent solution, put it aside for 24 hours after ultrasonic mutual dissolution, and obtain the natural gas rare earth nanometer energy-saving additive.
[0041] Add the above-mentioned additives to natural gas and do combustion exp...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology