[0026] A preparation method for a composite carrier material for a biological fluidized bed, comprising the steps of:
[0027] 1) Weigh diatomaceous earth, put it in 1mol / L sodium hydroxide solution, soak it at 40°C for 1h, take it out, wash it with water until the surface is neutral, and then calcinate it at 450°C for 2h; after cooling to room temperature Add it into 1mol / L hydrochloric acid solution, soak it at 40°C for 1h, take it out, wash it with water until the surface becomes neutral, calcinate it at 450°C for 1h, wash it with water and dry it to obtain purified diatomite;
[0028] 2) Take purified diatomite and KH570 and add them to anhydrous toluene at a mass ratio of 1:2, ultrasonically disperse them evenly, heat and reflux for 4-5 hours, and centrifuge after natural cooling, collect the solids, wash with ethanol, dry, and grind , to obtain modified diatomite powder;
[0029] 3) Add equal volumes of ethanol and water into the reaction flask respectively, under the p...
Embodiment 2
[0033] 1) Weigh diatomaceous earth, put it in 1mol / L sodium hydroxide solution, soak it at 40°C for 1h, take it out, wash it with water until the surface is neutral, and then calcinate it at 450°C for 2h; after cooling to room temperature Add it into 1mol / L hydrochloric acid solution, soak it at 40°C for 1h, take it out, wash it with water until the surface becomes neutral, calcinate it at 450°C for 1h, wash it with water and dry it to obtain purified diatomite;
[0034] 2) Add purified diatomite and KH570 into 50ml of anhydrous toluene at a mass ratio of 1:2, disperse evenly with ultrasound, heat and reflux for 4-5h, and centrifuge after natural cooling, collect the solids, wash with ethanol, and dry. Grinding to obtain modified diatomite powder;
[0035]3) Add equal volumes of ethanol and water into the reaction flask respectively, under the protection of nitrogen, add the modified diatomite powder into the reaction flask, stir to make it evenly dispersed, and then continue ...
Embodiment 3
[0038] Same as Example 2, the difference is that KH570 is replaced by KH560.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com