Environment-friendly pulping and papermaking composition, modifier and environment-friendly pulping and papermaking method
A technology for pulping and papermaking and modifiers, applied in pulp beating/refining methods, cellulose pulp post-treatment modification, papermaking, etc., can solve the problems of difficult to produce high-quality pulp, high alkali content in pulping wastewater, Papermaking wastewater is difficult to deal with, achieving the effect of low difficulty, high value and low energy consumption
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0035] The environment-friendly pulping and papermaking modifier of the present embodiment is made by mixing the following raw materials in mass percentage: 10% potassium hydroxide, 14% sodium sulfate, 8% calcium oxide, 7% hydrogen peroxide, 1% white rot fungus, and The amount is water.
[0036] Mix potassium hydroxide, sodium sulfate, calcium oxide, hydrogen peroxide, white rot fungus and water in a mixing tank for 1 hour to obtain the modifier. It is a colorless liquid, a small part of calcium peroxide precipitates at the bottom of the modifier.
Embodiment 2
[0038] The environment-friendly pulping and papermaking modifying agent of the present embodiment is made by mixing raw materials in the following mass percentages: 5% potassium hydroxide, 7% sodium sulfate, 5% calcium oxide, 5% hydrogen peroxide, 0.5% white rot fungus, and The amount is water.
[0039] Mix potassium hydroxide, sodium sulfate, calcium oxide, hydrogen peroxide, white rot fungus and water in a mixing tank for 2 hours to obtain the modifier.
Embodiment 3
[0041] The environment-friendly pulping and papermaking modifier of the present embodiment is made by mixing the raw materials in the following mass percentages: 7% potassium hydroxide, 10% sodium sulfate, 6% calcium oxide, 6% hydrogen peroxide, 0.8% white rot fungus, and The amount is water.
[0042] Mix potassium hydroxide, sodium sulfate, calcium oxide, hydrogen peroxide, white rot fungus and water in a mixing tank for 2 hours to obtain the modifier.
[0043] Two, the specific embodiment of the environment-friendly papermaking method of the present invention
PUM
| Property | Measurement | Unit |
|---|---|---|
| Length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com